Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Graphite
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1984) 33 (7): TS-424.
Published: 01 July 1984
Abstract
View articletitled, JESSOP TRUGLIDE: Graphitic Tool Steel, Type O6
View
PDF
for article titled, JESSOP TRUGLIDE: Graphitic Tool Steel, Type O6
JESSOP TRUGLIDE is a free-machining, oil-hardening too steel designed primarily for cold-work die applications. Free graphite in this steel gives it excellent machinability and outstanding resistance to galling and seizing in operation. Among its many uses are dies, gages, punches, arbors and bushings. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-424. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (1975) 24 (4): TS-287.
Published: 01 April 1975
Abstract
View articletitled, AISI TYPE O6: Graphitic Cold Work Oil Hardening Tool Steel
View
PDF
for article titled, AISI TYPE O6: Graphitic Cold Work Oil Hardening Tool Steel
AISI Type O6 is a free-machining, oil-hardening tool steel designed for cold-work dies. Because about one-third of its carbon is present as graphite, it has excellent machinability and exceptional resistance to galling and seizing. It is primarily used on drawing, forming and shaping operations where its self-lubricating quality is advantageous. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-287. Producer or source: Tool steel mills.