Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 186
Chemical and petrochemical processing equipment
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
Available to Purchase
Alloy Digest (2020) 69 (4): Ti-165.
Published: 01 April 2020
Abstract
View articletitled, ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
View
PDF
for article titled, ULBRICH TITANIUM GRADE 1 (UNS R50250): Unalloyed Commercially Pure Titanium
Ulbrich Titanium Grade 1 (UNS R50250) is an unalloyed commercially pure titanium. It is one of the softest and the most ductile of the commercially pure grades, and exhibits excellent formability. It has excellent corrosion resistance and is mainly used in marine and chemical industries where the parts are exposed to very harsh environments. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming. Filing Code: Ti-165. Producer or source: Ulbrich Stainless Steels & Special Metals, Inc.
Journal Articles
2120 MoN: Corrosion Resistant Nickel Alloy
Available to Purchase
Alloy Digest (2018) 67 (12): Ni-747.
Published: 01 December 2018
Abstract
View articletitled, 2120 MoN: Corrosion Resistant Nickel Alloy
View
PDF
for article titled, 2120 MoN: Corrosion Resistant Nickel Alloy
Alloy 2120 MoN has a wide range of applications in the chemical, petrochemical, and pharmaceutical industries, as well as in energy production and environmental technologies. This alloy is also referred to as Nicrofer 5821 hMoN. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, machining, and joining. Filing Code: Ni-747. Producer or source: VDM Metals International GmbH Germany.
Journal Articles
URANUS UR 2205Mo: Duplex Austenitic/Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2015) 64 (1): SS-1198.
Published: 01 January 2015
Abstract
View articletitled, URANUS UR 2205Mo: Duplex Austenitic/Ferritic Stainless Steel
View
PDF
for article titled, URANUS UR 2205Mo: Duplex Austenitic/Ferritic Stainless Steel
Uranus UR 2205Mo is a high chromium, molybdenum, and nitrogen alloy (PREN ≥ 35) that is very resistant to localized corrosion even in acidified oxidizing environments. The alloy has been used in the chemical industry. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1198. Producer or source: Industeel USA, LLC.
Journal Articles
FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
Available to Purchase
Alloy Digest (2013) 62 (1): SS-1133.
Published: 01 January 2013
Abstract
View articletitled, FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
View
PDF
for article titled, FERRALIUM 255-SD50: Ferritic/Austenitic Duplex Stainless Steel
Ferralium 255-SD50 has much higher strength than other commercially available superduplex alloys. Ferralium 255 is the original superduplex stainless steel, noted for its unique combination of mechanical properties and resistance to corrosion, erosion, and cavitation. It has especially low impurities giving improved corrosion resistance, and it is used extensively in the offshore and chemical industries. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and machining. Filing Code: SS-1133. Producer or source: Langley Alloys.
Journal Articles
NAS NW22: Corrosion-Resistant Nickel Alloy
Available to Purchase
Alloy Digest (2012) 61 (3): Ni-696.
Published: 01 March 2012
Abstract
View articletitled, NAS NW22: Corrosion-Resistant Nickel Alloy
View
PDF
for article titled, NAS NW22: Corrosion-Resistant Nickel Alloy
NAS NW22 is a Ni-Cr-Mo alloy with excellent corrosion resistance in both oxidizing and reducing atmospheres. In this alloy, carbide precipitation in the heat affected zone (HAZ) is suppressed, and corrosion resistance is improved by reducing the contents of C and Si. Based on these features, NAS NW22 is widely used in materials under severe environments such as chemical plants. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-696. Producer or source: Nippon Yakin Kogyo Company Ltd.
Journal Articles
NAS H840: Oxidation Resistant Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2011) 60 (4): SS-1088.
Published: 01 April 2011
Abstract
View articletitled, NAS H840: Oxidation Resistant Austenitic Stainless Steel
View
PDF
for article titled, NAS H840: Oxidation Resistant Austenitic Stainless Steel
NAS H840 is Ni-Cr-Fe alloy with excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces and petrochemical reactors. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1088. Producer or source: Nippon Yakin Kogyo Company Ltd.
Journal Articles
HPM MP35N-Lti: High Strength Cobalt Alloy
Available to Purchase
Alloy Digest (2010) 59 (12): Co-120.
Published: 01 December 2010
Abstract
View articletitled, HPM MP35N-Lti: High Strength Cobalt Alloy
View
PDF
for article titled, HPM MP35N-Lti: High Strength Cobalt Alloy
HPM MP35N-LTi is a nonmagnetic nickel-cobalt-chromium-molybdenum alloy that has excellent corrosion resistance, can obtain ultrahigh tensile strengths 2068 MPa (300 ksi) through work hardening and aging, and has good toughness and ductility. Applications include electrical components, springs, and instrument parts in medical, chemical, food processing and marine environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: CO-120. Producer or source: Hamilton Precision Metals.
Journal Articles
BOEHLER UDDEHOLM ALLOY BeCu172: Beryllium Copper Mold Material
Available to Purchase
Alloy Digest (2010) 59 (4): Cu-781.
Published: 01 April 2010
Abstract
View articletitled, BOEHLER UDDEHOLM ALLOY BeCu172: Beryllium Copper Mold Material
View
PDF
for article titled, BOEHLER UDDEHOLM ALLOY BeCu172: Beryllium Copper Mold Material
Boehler Uddeholm alloy BeCu172 is a high-strength beryllium copper mold with high thermal conductivity. BeCu Alloy 172 can be supplied in the high-hard (HH) condition at approximately 40 HRC and in the low-hard (LH) condition at approximately 30 HRC. This alloy is used for applications such as pinch-offs and neck rings for blow molds, cores, and inserts in injection molds and injection nozzles and manifolds for hot runner systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-781. Producer or source: Böhler-Uddeholm Corporation.
Journal Articles
BOEHLER L330 VMR: Nickel-Base Alloy
Available to Purchase
Alloy Digest (2006) 55 (11): Ni-642.
Published: 01 November 2006
Abstract
View articletitled, BOEHLER L330 VMR: Nickel-Base Alloy
View
PDF
for article titled, BOEHLER L330 VMR: Nickel-Base Alloy
Boehler L330 VMR is a Ni-Mo-Cr-W alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution control, industrial and municipal waste treatment, and pulp and paper production. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Ni-642. Producer or source: Böhler-Uddeholm Specialty Metals Inc.
Journal Articles
ALLVAC Ti-15Mo: Beta-Rich Alpha-Beta Alloy
Available to Purchase
Alloy Digest (2005) 54 (7): Ti-136.
Published: 01 July 2005
Abstract
View articletitled, ALLVAC Ti-15Mo: Beta-Rich Alpha-Beta Alloy
View
PDF
for article titled, ALLVAC Ti-15Mo: Beta-Rich Alpha-Beta Alloy
Allvac Ti-15Mo is a metastable beta alloy melted in a vacuum arc remelting (VAR) furnace to minimize segregation. The alloy has a unique combination of properties and is used in the medical, chemical, and aerospace industries. This datasheet provides information on composition. Filing Code: TI-136. Producer or source: Allvac, an Allegheny Technologies Company.
Journal Articles
ATI 425: High-Strength Titanium Alloy
Available to Purchase
Alloy Digest (2004) 53 (7): Ti-133.
Published: 01 July 2004
Abstract
View articletitled, ATI 425: High-Strength Titanium Alloy
View
PDF
for article titled, ATI 425: High-Strength Titanium Alloy
ATI 425 was originally developed for hot-rolled armor plate to provide ballistic protection comparable to Ti-6Al-4V and has been evaluated against a variety of projectile threats for use as armor. While processing the alloy for armor plate applications, it was observed that the material exhibited very good hot workability, permitting a more lenient window of processing parameters than necessary for Ti-6Al-4V. Versatility then expanded, and applications now exist in the chemical process industry (CPI) and in the aerospace industry. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance. Filing Code: TI-133. Producer or source: ATI Wah Chang, Allegheny Technologies. Originally published March 2004, revised July 2004.
Journal Articles
CARLSON ALLOY 317L, 317L 4, and 317L 4N: Corrosion-Resistant Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2002) 51 (3): SS-846.
Published: 01 March 2002
Abstract
View articletitled, CARLSON ALLOY 317L, 317L 4, and 317L 4N: Corrosion-Resistant Austenitic Stainless Steel
View
PDF
for article titled, CARLSON ALLOY 317L, 317L 4, and 317L 4N: Corrosion-Resistant Austenitic Stainless Steel
Carlson alloys 317L, 317L 4, and 317L 4N are a family of superior corrosion-resistant austenitic stainless steels for service in severe envi-ronments. They maintain tensile and creep-rupture strength at elevated temperatures and are resistant to intergranular attack. These alloys are widely used in air-pollution control systems, pulp and paper plants, and chemical and petrochemical processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-846. Producer or source: G.O. Carlson Inc.
Journal Articles
TIMETAL 75A: Commercially Pure Titanium
Available to Purchase
Alloy Digest (2001) 50 (10): Ti-121.
Published: 01 October 2001
Abstract
View articletitled, TIMETAL 75A: Commercially Pure Titanium
View
PDF
for article titled, TIMETAL 75A: Commercially Pure Titanium
TIMETAL 75A is the highest-strength commercially pure sheet grade. It is readily formed at room temperature, but warm forming is frequently used to reduce springback and the power requirements. Complex forms must be made by warm forming. This material is weldable by both electrical resistance and fusion procedures, although the latter methods can be used only if the material is protected from atmospheric contamination. Machining requires a rigid tool setup, slow speed, heavy feed, sharp tools, and adequate coolant. This material is used in aircraft and chemical process applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-121. Producer or source: Timet.
Journal Articles
TIMETAL 50A: Commercially Pure Titanium
Available to Purchase
Alloy Digest (2001) 50 (9): Ti-120.
Published: 01 September 2001
Abstract
View articletitled, TIMETAL 50A: Commercially Pure Titanium
View
PDF
for article titled, TIMETAL 50A: Commercially Pure Titanium
TIMETAL 50A is a commercially pure titanium alloy with a minimum tensile strength of 345 MPa (50 ksi). It is readily formed at room temperature, although complex shapes must be warm formed for satisfactory results. This material is weldable by both electrical resistance and fusion procedures, although the latter methods can be used only if the material is protected from atmospheric contamination. This grade is used in airframe and chemical process applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-120. Producer or source: Timet.
Journal Articles
GIBSON TUBE DUPLEX 2205: Ferritic/Austenitic Duplex Stainless Steel
Available to Purchase
Alloy Digest (2001) 50 (1): SS-813.
Published: 01 January 2001
Abstract
View articletitled, GIBSON TUBE DUPLEX 2205: Ferritic/Austenitic Duplex Stainless Steel
View
PDF
for article titled, GIBSON TUBE DUPLEX 2205: Ferritic/Austenitic Duplex Stainless Steel
Duplex alloy 2205 is a nitrogen-enhanced, ferritic-austenitic stainless steel. It has high resistance to stress-corrosion cracking (SCC); pitting; crevice and general corrosion. It has roughly twice the yield strength of austenitic stainless grades and it has good weldability. Some uses include heat exchangers, downhole instrument tubing, and applications in desalination plants. All Gibson Tube Duplex 2205 products meet the tighter composition limits of UNS S32205 to enhance corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: SS-813. Producer or source: Gibson Tube.
Journal Articles
J&L TYPE 2205: Duplex Stainless Steel
Available to Purchase
Alloy Digest (2000) 49 (1): SS-773.
Published: 01 January 2000
Abstract
View articletitled, J&L TYPE 2205: Duplex Stainless Steel
View
PDF
for article titled, J&L TYPE 2205: Duplex Stainless Steel
J and L 2205 is a ferritic-austenitic duplex stainless steel. It resists stress-corrosion cracking very well and has good pitting and general corrosion resistance. Its high strength and stress-corrosion resisting characteristics are a reflection of its duplex microstructure. Its uses include pipe, tubing, tanks, and heat exchangers for the chemical industries. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-773. Producer or source: J & L Specialty Steel Inc.
Journal Articles
CRUCIBLE P/M 625M: Heat Treatable Nickel-Base CRA
Available to Purchase
Alloy Digest (1999) 48 (6): Ni-554.
Published: 01 June 1999
Abstract
View articletitled, CRUCIBLE P/M 625M: Heat Treatable Nickel-Base CRA
View
PDF
for article titled, CRUCIBLE P/M 625M: Heat Treatable Nickel-Base CRA
Crucible P/M 625M is a powder metallurgy produced alloy where the composition meets both high-strength and corrosion-resistance requirements. P/M 625M is a candidate for critical service industries such as nuclear power, chemical process, pulp, paper, and oil fields. This datasheet provides information on composition, microstructure, and hardness as well as fracture toughness. It also includes information on low temperature performance and corrosion resistance as well as heat treating and powder metal forms. Filing Code: Ni-554. Producer or source: Crucible Compaction Metals.
Journal Articles
ALLEGHENY LUDLUM TYPE 310: Heat Resistant Austenitic Stainless Steel
Available to Purchase
Alloy Digest (1998) 47 (6): SS-719.
Published: 01 June 1998
Abstract
View articletitled, ALLEGHENY LUDLUM TYPE 310: Heat Resistant Austenitic Stainless Steel
View
PDF
for article titled, ALLEGHENY LUDLUM TYPE 310: Heat Resistant Austenitic Stainless Steel
Allegheny Ludlum Type 310 is an austenitic chromium-nickel steel with high heat resisting properties. It is recommended for furnace equipment, heat treating boxes, burners, heat recovery systems, jet engine components, and heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-719. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
UCI 193: Heat Resistant Cast Stainless Steel
Available to Purchase
Alloy Digest (1998) 47 (4): SS-714.
Published: 01 April 1998
Abstract
View articletitled, UCI 193: Heat Resistant Cast Stainless Steel
View
PDF
for article titled, UCI 193: Heat Resistant Cast Stainless Steel
UCI-193 is an HP + Nb grade material for use in the petrochemical arena. The HP + Nb grade resists carburization, oxidation, and creep up to 1093 C (2000 F). This improvement over the HP grade, UCI-190 (Alloy Digest SS-689, July 1997), is due to the addition of niobium. UCI-190 has been used for many years for consistent and predictable results in high temperature applications. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-714. Producer or source: Ultra-Cast Inc.
Journal Articles
ALLOY 0Cr25Ni6Mo3CuN: Ferritic/Austenitic Duplex Stainless Steel
Available to Purchase
Alloy Digest (1998) 47 (2): SS-706.
Published: 01 February 1998
Abstract
View articletitled, ALLOY 0Cr25Ni6Mo3CuN: Ferritic/Austenitic Duplex Stainless Steel
View
PDF
for article titled, ALLOY 0Cr25Ni6Mo3CuN: Ferritic/Austenitic Duplex Stainless Steel
ALLOY 0Cr25Ni6Mo3CuN is one of four grades of duplex stainless steel that were developed and have found wide applications in China since 1980. In oil refinement and the petrochemical processing industries, they have substituted for austenitic stainless steels in many types of equipment, valves, and pump parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS-706. Producer or source: Central Iron & Steel Research Institute.
1