Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-7 of 7
Engine cylinder heads
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1986) 35 (10): Al-272.
Published: 01 October 1986
Abstract
View articletitled, UNS A02220: Aluminum Foundry Alloy
View
PDF
for article titled, UNS A02220: Aluminum Foundry Alloy
UNS No. A02220 is an age-hardenable aluminum casting alloy. It is hard and wear resistant and has good strength at elevated temperatures. It has good foundry characteristics in many respects and is produced as sand and permanent-mold castings. Among its applications are bushings, automotive cylinder heads and pistons. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-272. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1985) 34 (3): Al-255.
Published: 01 March 1985
Abstract
View articletitled, ALUMINUM 213.0: Permanent Mold Casting Alloy
View
PDF
for article titled, ALUMINUM 213.0: Permanent Mold Casting Alloy
ALUMINUM 213.0 is an aluminum-base alloy that is used for permanent-mold castings. It is characterized by good castability, excellent machinability, moderate strength and fair weldability. Among its uses are pressure-tight castings and automotive cylinder heads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Al-255. Producer or source: Various aluminum companies. See also Alloy Digest Al-246, July 1983.
Journal Articles
Alloy Digest (1983) 32 (7): Al-246.
Published: 01 July 1983
Abstract
View articletitled, ALUMINUM 213.0: Permanent Mold Casting Alloy
View
PDF
for article titled, ALUMINUM 213.0: Permanent Mold Casting Alloy
ALUMINUM 213.0 is a permanent-mold casting alloy that has good castability, moderate strength and excellent machinability. It also has good pressure tightness. Its applications include automotive cylinder heads and timing gears. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Al-246. Producer or source: Various aluminum companies. See also Alloy Digest Al-255, March 1985.
Journal Articles
Alloy Digest (1982) 31 (1): Al-235.
Published: 01 January 1982
Abstract
View articletitled, ALUMINUM 355.0: Heat Treatable Aluminum Casting Alloy
View
PDF
for article titled, ALUMINUM 355.0: Heat Treatable Aluminum Casting Alloy
ALUMINUM 355.0 is a general-purpose, high-strength casting alloy containing silicon and copper as the major alloying elements. Its casting characteristics are excellent and it is recommended for pressure-tight castings. It can be age hardened and has good resistance to corrosion. Among its uses are housings, cylinder heads and propeller gear boxes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-235. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1979) 28 (5): Al-130.
Published: 01 May 1979
Abstract
View articletitled, ALUMINUM 2018: Aluminum Forging Alloy
View
PDF
for article titled, ALUMINUM 2018: Aluminum Forging Alloy
ALUMINUM 2018 is an age-hardenable aluminum forging alloy characterized by relatively high tensile and yield strengths along with fairly good ductility. It has good elevated-temperature properties. Its applications include engine pistons and engine cylinder heads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-130. Producer or source: Various aluminum companies. Originally published October 1963, revised May 1979.
Journal Articles
Alloy Digest (1969) 18 (6): Al-187.
Published: 01 June 1969
Abstract
View articletitled, ALUMINUM A140: Aluminum Casting Alloy
View
PDF
for article titled, ALUMINUM A140: Aluminum Casting Alloy
Aluminum A-140 is a non-heat treatable casting alloy having high tensile and fatigue strength at elevated temperatures to 600 F. It is recommended for engine cylinder heads, aircraft and missile components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-187. Producer or source: Aluminum Company of America.
Journal Articles
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
Abstract
View articletitled, ALUMINUM A357: Sand and Permanent Mold Casting Alloy
View
PDF
for article titled, ALUMINUM A357: Sand and Permanent Mold Casting Alloy
Aluminum A357 is a high strength, pressure tight sand and permanent mold aluminum casting alloy. It is age-hardenable. It is recommended for cast gear cases, cylinder heads, transmission cases and strong structural castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-163. Producer or source: Aluminum Company of America.