Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 118
Thermal resistance
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
CRYODUR 2833: Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (10): TS-777.
Published: 01 October 2019
Abstract
View articletitled, CRYODUR 2833: Cold-Work Tool Steel
View
PDF
for article titled, CRYODUR 2833: Cold-Work Tool Steel
Cryodur 2833 is a wear-resistant water-hardening steel with resistance to overheating. Applications include cold heading dies; first and finish upsetting punches; cold stamps; dies for the manufacturing of screws, rivets, and bolts; and compression pistons. This datasheet provides information on composition and physical properties. It also includes information on heat treating. Filing Code: TS-777. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
MANAURITE XMR: High-Temperature Nickel Alloy
Available to Purchase
Alloy Digest (2019) 68 (1): Ni-749.
Published: 01 January 2019
Abstract
View articletitled, MANAURITE XMR: High-Temperature Nickel Alloy
View
PDF
for article titled, MANAURITE XMR: High-Temperature Nickel Alloy
Manaurite XMR is a heat resistant alloy for hydrocarbon processing. It is a modified version of Manaurite XM (Alloy Digest Ni-748, December 2018) designed to withstand creep elongation at high temperature, while also being able to be welded after aging. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on joining. Filing Code: Ni-749. Producer or source: Manoir Pîtres.
Journal Articles
XAR 400W: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (1): SA-836.
Published: 01 January 2019
Abstract
View articletitled, XAR 400W: Wear-Resistant Structural Steel
View
PDF
for article titled, XAR 400W: Wear-Resistant Structural Steel
XAR 400W is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear-resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. It is heat resistant up to 400 deg C. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-836. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
MTEK 25-35MA: High-Temperature Austenitic Casting Alloy
Available to Purchase
Alloy Digest (2016) 65 (9): SS-1249.
Published: 01 September 2016
Abstract
View articletitled, MTEK 25-35MA: High-Temperature Austenitic Casting Alloy
View
PDF
for article titled, MTEK 25-35MA: High-Temperature Austenitic Casting Alloy
MTEK 25-35MA is a solid solution microalloyed Fe-Ni-Cr-Nb casting alloy with good high-temperature creep strength. It is intended for use in pyrolysis cracker furnaces. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: SS-1249. Producer or source: MetalTek International. Originally published July 2016, revised September 2016.
Journal Articles
NAS 660: Heat Resistant Stainless Steel
Available to Purchase
Alloy Digest (2014) 63 (11): SS-1189.
Published: 01 November 2014
Abstract
View articletitled, NAS 660: Heat Resistant Stainless Steel
View
PDF
for article titled, NAS 660: Heat Resistant Stainless Steel
NAS 660 is a Ni-Cr stainless steel alloy with excellent heat resistance. The alloy is used for its high strength at high temperatures. The alloy is a precipitation-hardening material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: SS-1189. Producer or source: Nippon Yakin Kogyo Company Ltd.
Journal Articles
KUBOTA ALLOY KHR35AF: Heat Resistant Austenitic Stainless Castings
Available to Purchase
Alloy Digest (2014) 63 (9): SS-1184.
Published: 01 September 2014
Abstract
View articletitled, KUBOTA ALLOY KHR35AF: Heat Resistant Austenitic Stainless Castings
View
PDF
for article titled, KUBOTA ALLOY KHR35AF: Heat Resistant Austenitic Stainless Castings
Kubota alloy KHR35AF is a heat resisting wholly austenitic stainless steel casting for ethylene pyrolysis. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep. It also includes information on casting and joining. Filing Code: SS-1184. Producer or source: Kubota Metal Corporation.
Journal Articles
MC ALLOY: Nickel-Based Corrosion Resistant Alloy
Available to Purchase
Alloy Digest (2014) 63 (7): Ni-713.
Published: 01 July 2014
Abstract
View articletitled, MC ALLOY: Nickel-Based Corrosion Resistant Alloy
View
PDF
for article titled, MC ALLOY: Nickel-Based Corrosion Resistant Alloy
MC Alloy is composed mostly of nickel with 45% chromium. The alloy has outstanding properties for both corrosion and heat resistance. This datasheet provides information on composition. It also includes information on corrosion resistance as well as forming. Filing Code: Ni-713. Producer or source: Hitachi Metals MMC Superalloy Ltd.
Journal Articles
BÖHLER W303 ISODISC: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2013) 62 (12): TS-724.
Published: 01 December 2013
Abstract
View articletitled, BÖHLER W303 ISODISC: Hot Work Tool Steel
View
PDF
for article titled, BÖHLER W303 ISODISC: Hot Work Tool Steel
Böhler (or Boehler) W303 ISODISC is a hot work tool steel with outstanding hot tensile properties, high retention of hardness, good toughness, and resistance to heat checking. W303 ISODISC is a special grade with improved homogeneity and increased toughness. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-724. Producer or source: Böhler Edelstahl GmbH.
Journal Articles
KUBOTA ALLOY HF: Heat-Resistant Stainless Casting
Available to Purchase
Alloy Digest (2012) 61 (2): SS-1115.
Published: 01 February 2012
Abstract
View articletitled, KUBOTA ALLOY HF: Heat-Resistant Stainless Casting
View
PDF
for article titled, KUBOTA ALLOY HF: Heat-Resistant Stainless Casting
Kubota Alloy HF is a heat-resisting stainless steel casting suitable for long-term service at temperatures between 538-871 deg C (1000-1600 deg F). It is frequently used as an alternative to the 2.25%Cr-1%Mo steels due to its greater ease of fabrication. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance as well as casting and joining. Filing Code: SS-1115. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
KUBOTA ALLOY HD: Heat Resistant Stainless Casting
Available to Purchase
Alloy Digest (2011) 60 (12): SS-1110.
Published: 01 December 2011
Abstract
View articletitled, KUBOTA ALLOY HD: Heat Resistant Stainless Casting
View
PDF
for article titled, KUBOTA ALLOY HD: Heat Resistant Stainless Casting
Kubota Alloy HD (UNS J93005) is a heat-resisting stainless steel casting alloy suitable for long-term service at temperatures up to 1095 deg C (2000 deg F). The nearest wrought equivalent is type 327. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on corrosion resistance as well as casting and joining. Filing Code: SS-1110. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
KUBOTA ALLOY HC: Heat Resistant Stainless Casting
Available to Purchase
Alloy Digest (2010) 59 (5): SS-1065.
Published: 01 May 2010
Abstract
View articletitled, KUBOTA ALLOY HC: Heat Resistant Stainless Casting
View
PDF
for article titled, KUBOTA ALLOY HC: Heat Resistant Stainless Casting
Kubota Alloy HC is a heat resisting stainless steel casting suitable for long term service at temperatures up to 1093 deg C (2000 deg F). This alloy can maintain resistance to sulfur bearing environments up to 1093 deg C (2000 deg F). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as casting and joining. Filing Code: SS-1065. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
UGINOX R24-13S: Heat Resisting Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2010) 59 (5): SS-1063.
Published: 01 May 2010
Abstract
View articletitled, UGINOX R24-13S: Heat Resisting Austenitic Stainless Steel
View
PDF
for article titled, UGINOX R24-13S: Heat Resisting Austenitic Stainless Steel
UGINOX R24-13S is an austenitic heat resistant stainless steel with good oxidation resistance. The alloy is frequently used in the heat treating industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and joining. Filing Code: SS-1063. Producer or source: Arcelor Stainless USA and Ugine & ALZ.
Journal Articles
KUBOTA ALLOY HI: Heat-Resistant Stainless Casting
Available to Purchase
Alloy Digest (2010) 59 (2): SS-1052.
Published: 01 February 2010
Abstract
View articletitled, KUBOTA ALLOY HI: Heat-Resistant Stainless Casting
View
PDF
for article titled, KUBOTA ALLOY HI: Heat-Resistant Stainless Casting
Kubota Alloy HI is a heat-resistant stainless steel casting suitable for long-term service at temperatures up to 1105 deg C (2025 deg F). Furnace skids and rail, conveyor roll assemblies, lead pots and retorts are typical applications. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on corrosion resistance as well as casting and joining. Filing Code: SS-1052. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
COLMONOY NO. 63HV: Hard-Surfacing Alloy
Available to Purchase
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
Abstract
View articletitled, COLMONOY NO. 63HV: Hard-Surfacing Alloy
View
PDF
for article titled, COLMONOY NO. 63HV: Hard-Surfacing Alloy
Colmonoy No. 63HV is a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat, and galling. The hardness of Colmonoy 63HV ranges to 58–61 HRC, and it is resistant to abrasion. Colmonoy 63HV is sized exclusively for high-velocity oxygen-fuel thermal spray systems. This datasheet provides information on composition. It also includes information on heat treating, surface treatment, and powder metal forms. Filing Code: Ni-665. Producer or source: Wall Colmonoy Corporation.
Journal Articles
COLMONOY NO. 43HV: Hard Surfacing Alloy
Available to Purchase
Alloy Digest (2008) 57 (7): Ni-664.
Published: 01 July 2008
Abstract
View articletitled, COLMONOY NO. 43HV: Hard Surfacing Alloy
View
PDF
for article titled, COLMONOY NO. 43HV: Hard Surfacing Alloy
Colmonoy No. 43HV comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat, and galling. Deposits that have moderate hardness have increased ductility and slightly less resistance to abrasion than Colmonoy 53HV. Deposits can be finished by grinding or machined with carbide tooling. Colmonoy No. 43HV is supplied as an atomized powder specially sized for application with high-velocity oxygen fuel (HVOF) systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance and surface qualities as well as heat treating and surface treatment. Filing Code: Ni-664. Producer or source: Wall Colmonoy Corporation.
Journal Articles
UGINOX R25-20: Heat-Resistant Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2008) 57 (3): SS-1009.
Published: 01 March 2008
Abstract
View articletitled, UGINOX R25-20: Heat-Resistant Austenitic Stainless Steel
View
PDF
for article titled, UGINOX R25-20: Heat-Resistant Austenitic Stainless Steel
Uginox R25-20 is an austenitic heat-resistant stainless steel with good oxidation resistance due to its 25% Cr content. The alloy is frequently used in the heat treating industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: SS-1009. Producer or source: Arcelor Stainless USA.
Journal Articles
KUBOTA HK40 and HK50: Heat-Resistant Castings
Available to Purchase
Alloy Digest (2007) 56 (10): SS-998.
Published: 01 October 2007
Abstract
View articletitled, KUBOTA HK40 and HK50: Heat-Resistant Castings
View
PDF
for article titled, KUBOTA HK40 and HK50: Heat-Resistant Castings
Kubota alloys HK40 and HK50 are austenitic Fe-Cr-Ni alloys that have been standard heat-resistant materials for more than four decades. With moderately high temperature strength, oxidation resistance, and carburization resistance the alloys are used in a wide variety of industrial applications. HK 50 has slightly higher carbon content. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on casting, heat treating, machining, and joining. Filing Code: SS-998. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
CRUCIBLE CPM 1V: Powder Metallurgy Medium-Carbon High-Alloy Tool Steel
Available to Purchase
Alloy Digest (2004) 53 (9): TS-605.
Published: 01 September 2004
Abstract
View articletitled, CRUCIBLE CPM 1V: Powder Metallurgy Medium-Carbon High-Alloy Tool Steel
View
PDF
for article titled, CRUCIBLE CPM 1V: Powder Metallurgy Medium-Carbon High-Alloy Tool Steel
CPM 1V is a powder metallurgically produced high-vanadium cold-work tool steel. It is an upgrade to H13 with higher hardness and better temper resistance for longer die life. The alloy also has better heat resistance and higher hardness than H19. This datasheet provides information on composition, physical properties, microstructure, and elasticity as well as fatigue. It also includes information on heat treating, machining, and powder metal forms. Filing Code: TS-605. Producer or source: Crucible Service Centers.
Journal Articles
UCI-390: Cast Heat Resistant Grade
Available to Purchase
Alloy Digest (2001) 50 (6): SS-824.
Published: 01 June 2001
Abstract
View articletitled, UCI-390: Cast Heat Resistant Grade
View
PDF
for article titled, UCI-390: Cast Heat Resistant Grade
UCI-390 is the casting grade equivalent to alloy UNS N08811. The alloy is stable at high temperatures, weldable, and resistant to thermal gradients. UCI-390 is widely used in thermal shock applications. It is corrosion resistant in air, oxidizing and reducing flue gases, carburizing gases, salts, and molten metals. The alloy performs satisfactorily up to 1150 C (2100 F) in oxidizing atmospheres and up to 1095 C (2000 F) in reducing atmospheres, provided that limiting creep-stress value are not exceeded. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-824. Producer or source: Ultra-Cast Inc.
Journal Articles
BOEHLER W302 ISOBLOC: Hot-Work Tool Steel
Available to Purchase
Alloy Digest (2000) 49 (8): TS-579.
Published: 01 August 2000
Abstract
View articletitled, BOEHLER W302 ISOBLOC: Hot-Work Tool Steel
View
PDF
for article titled, BOEHLER W302 ISOBLOC: Hot-Work Tool Steel
Boehler W302 ISOBLOC is a premium grade H13 tool steel with a good combination of toughness, heat-checking resistance, temperature resistance, and high-temperature strength. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as heat treating, machining, joining, and surface treatment. Filing Code: TS-579. Producer or source: Böhler.