Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 5977
Physical properties
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
SAE 1064, SAE 1065, ISO CS65, JIS S65CM, JIS S65C, JIS S65C-CSP: Wrought High-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2025) 74 (1): CS-270.
Published: 06 March 2025
Abstract
View articletitled, SAE 1064, SAE 1065, ISO CS65, JIS S65CM, JIS S65C, JIS S65C-CSP: Wrought High-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1064, SAE 1065, ISO CS65, JIS S65CM, JIS S65C, JIS S65C-CSP: Wrought High-Carbon Non-Alloy Steels
1064, 1065, CS65, S65CM, S65C, and S65C-CSP are wrought high-carbon non-alloy steels that are typically used in the cold reduced, patented and cold drawn, quenched and tempered, or austempered condition. These steels are widely used for highly stressed parts that require higher strength levels than can be achieved with lower carbon grades. They are also used for applications where the higher carbon is needed to improve wear characteristics. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: CS-270. Producer or source: Heat Treater’s Guide Data Sheet.
Journal Articles
SAE 8620, SAE 8620H, SAE 8620RH, CEN ISO 20NiCrMo2-2, JIS SNCM220: Wrought Low-Carbon, Nickel-Chromium-Molybdenum, Low Alloy Steels
Available to Purchase
Alloy Digest (2025) 74 (1): SA-879.
Published: 06 March 2025
Abstract
View articletitled, SAE 8620, SAE 8620H, SAE 8620RH, CEN ISO 20NiCrMo2-2, JIS SNCM220: Wrought Low-Carbon, Nickel-Chromium-Molybdenum, Low Alloy Steels
View
PDF
for article titled, SAE 8620, SAE 8620H, SAE 8620RH, CEN ISO 20NiCrMo2-2, JIS SNCM220: Wrought Low-Carbon, Nickel-Chromium-Molybdenum, Low Alloy Steels
8620, 8620H, 8620RH, 20NiCrMo2-2, 20NiCrMoS2-2, SNCM220, and SNCM220H are wrought, low-carbon, nickel-chromium-molybdenum, low alloy steels that are typically used in the carburized or carbonitrided, and subsequently quench hardened, and tempered condition. In general, these steels are intended for the manufacture of small- and medium-sized case-hardened parts that require a high hardness, high carbon, martensitic case with good wear and fatigue resistance, and a strong and tough low-carbon steel core. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: SA-879. Producer or source: Heat Treater’s Guide Data Sheet.
Journal Articles
SAE 1016, CEN C16, ISO C16: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2024) 73 (4): CS-269.
Published: 01 December 2024
Abstract
View articletitled, SAE 1016, CEN C16, ISO C16: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1016, CEN C16, ISO C16: Wrought Low-Carbon Non-Alloy Steels
1016, C16E, and C16R are wrought low-carbon (carbon = 0.12–0.18%) non-alloy steels that are used in the as-rolled, annealed, normalized, or cold worked condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-medium strength, excellent cold formability, and excellent weldability are required. These steels may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on low and high temperature performance as well as forming and heat treating. Filing Code: CS-269. Producer or source: Heat Treater's Guide Data Sheet.
Journal Articles
DEUTSCHE EDELSTAHLWERKE CRYODUR 2381: Alloy Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2024) 73 (4): TS-841.
Published: 01 December 2024
Abstract
View articletitled, DEUTSCHE EDELSTAHLWERKE CRYODUR 2381: Alloy Cold-Work Tool Steel
View
PDF
for article titled, DEUTSCHE EDELSTAHLWERKE CRYODUR 2381: Alloy Cold-Work Tool Steel
Deutsche Edelstahlwerke Cryodur 2381 is a high-carbon, silicon-molybdenum-vanadium alloy cold-work tool steel. This high-tensile special steel exhibits good resistance to twisting. This datasheet provides information on composition, physical properties, and hardness as well as fatigue. It also includes information on heat treating. Filing Code: TS-841. Producer or source: Deutsche Edelstahlwerke Specialty Steel.
Journal Articles
CLEVELAND-CLIFFS 18 SR: Ferritic Stainless Steel
Available to Purchase
Alloy Digest (2024) 73 (4): SS-1367.
Published: 01 December 2024
Abstract
View articletitled, CLEVELAND-CLIFFS 18 SR: Ferritic Stainless Steel
View
PDF
for article titled, CLEVELAND-CLIFFS 18 SR: Ferritic Stainless Steel
Cleveland-Cliffs 18 SR is a ferritic stainless steel that is especially valuable for applications requiring high-temperature scaling resistance. Its properties, under cyclic conditions, are superior to those of types 409, 430, 304, 309, and 310 stainless steels. In addition, it is more economical than many of the stainless steels that are intended for high temperature applications. Unlike many of the straight chromium alloys, Cleveland-Cliffs 18 SR is readily welded by conventional methods. It is not subject to troublesome embrittlement or loss of corrosion resistance in the heat-affected zone. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low temperature performance, high temperature performance, and corrosion resistance as well as forming and joining. Filing Code: SS-1367. Producer or source: Cleveland-Cliffs Inc.
Journal Articles
SAE 1012, JIS S12C: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2024) 73 (3): CS-268.
Published: 01 September 2024
Abstract
View articletitled, SAE 1012, JIS S12C: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1012, JIS S12C: Wrought Low-Carbon Non-Alloy Steels
1012 and S12C are wrought low-carbon (carbon = 0.10–0.15 percent) non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. These steels are characterized by low strength, high ductility, excellent cold formability, and excellent weldability. Within the carbon range of these steel grades, strength and hardness will increase with increase in carbon content and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. Grades 1012 and S12C are widely used for lightly stressed parts that require higher strength levels than can be achieved by the lower carbon grades and for applications where cold formability is the primary requisite. They are less expensive than 1008 and can be used when the requirements for cold forming are less exacting. 1012 and S12C may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on low and high temperature performance as well as forming and heat treating. Filing Code: CS-268. Producer or source: Heat Treater's Guide.
Journal Articles
AUSTRAL WRIGHT 70-30 Brass (UNS C26000): Cu-30Zn Alloy
Available to Purchase
Alloy Digest (2024) 73 (3): Cu-944.
Published: 01 September 2024
Abstract
View articletitled, AUSTRAL WRIGHT 70-30 Brass (UNS C26000): Cu-30Zn Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 70-30 Brass (UNS C26000): Cu-30Zn Alloy
Austral Wright C26000 (70-30 Brass) is a copper-zinc alloy. It has the distinctive clear bright yellow color normally associated with brass. Austral Wright C26000 possesses an excellent combination of strength and ductility. This grade is the most widely available copper alloy in the sheet form. It is often used where its deep drawing qualities are needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-944. Producer or source: Austral Wright Metals.
Journal Articles
AUBERT & DUVAL PER72: Nickel-Base Superalloy
Available to Purchase
Alloy Digest (2024) 73 (3): Ni-787.
Published: 01 September 2024
Abstract
View articletitled, AUBERT & DUVAL PER72: Nickel-Base Superalloy
View
PDF
for article titled, AUBERT & DUVAL PER72: Nickel-Base Superalloy
Aubert and Duval PER72 (NiCr18Co15TiMoAI alloy) is a precipitation hardening, nickel-base superalloy. The alloy is solid solution strengthened by additions of chromium, cobalt, molybdenum, and tungsten, while additions of titanium and aluminum provide precipitation strengthening. Aubert & Duval PER72 combines high strength with metallurgical stability as demonstrated by excellent impact strength retention after long exposures at elevated temperatures. It also exhibits good oxidation resistance, as well as excellent resistance to sulfide corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on low temperature performance, high temperature performance, and corrosion resistance as well as forming and heat treating. Filing Code: Ni-787. Producer or source: Aubert & Duval S.A. (a member of the Eramet Group).
Journal Articles
SAE 1006: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2024) 73 (2): CS-267.
Published: 01 June 2024
Abstract
View articletitled, SAE 1006: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1006: Wrought Low-Carbon Non-Alloy Steels
1006 is a wrought low-carbon (carbon ≤ 0.08%) non-alloy steel that is used in the as rolled, annealed, normalized, or cold worked condition. This steel is characterized by low strength, high ductility, excellent cold formability, and excellent weldability. Within the carbon range of this steel grade, both strength and hardness will increase with increase in carbon and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1006 is widely used for lightly stressed parts where cold formability or drawability is the primary requisite. In general, it is not intended for heat treatment after cold working. 1006 may, however, be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-267. Producer or source: Heat Treater's Guide.
Journal Articles
ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
Available to Purchase
Alloy Digest (2024) 73 (2): CI-109.
Published: 01 June 2024
Abstract
View articletitled, ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
View
PDF
for article titled, ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
ACO Eurobar EN-GJS-400-18C-LT is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 18%. It has a tensile strength exceeding that of the highest-tensile-strength grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance as well as casting, heat treating, and machining. Filing Code: CI-109. Producer or source: ACO Eurobar GmbH.
Journal Articles
DEUTSCHE EDELSTAHLWERKE CRYODUR 2362: Alloy Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2024) 73 (2): TS-840.
Published: 01 June 2024
Abstract
View articletitled, DEUTSCHE EDELSTAHLWERKE CRYODUR 2362: Alloy Cold-Work Tool Steel
View
PDF
for article titled, DEUTSCHE EDELSTAHLWERKE CRYODUR 2362: Alloy Cold-Work Tool Steel
Deutsche Edelstahlwerke Cryodur 2362 is a high-carbon, chromium-molybdenum-vanadium alloy cold-work tool steel with high tempering resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information on wear resistance as well as forming and heat treating. Filing Code: TS-840. Producer or source: Deutsche Edelstahlwerke Specialty Steel GmbH.
Journal Articles
VDM 40 B: Alloy for Electrical Heating Elements
Available to Purchase
Alloy Digest (2024) 73 (1): SS-1366.
Published: 01 March 2024
Abstract
View articletitled, VDM 40 B: Alloy for Electrical Heating Elements
View
PDF
for article titled, VDM 40 B: Alloy for Electrical Heating Elements
VDM 40 B is an austenitic iron-nickel-chromium-silicon-lanthanum alloy that is suitable for heating elements. It is characterized by excellent oxidation resistance, high resistivity, good sag resistance, and superior mechanical properties at high temperatures in comparison to other heating element alloys. VDM 40 B is less expensive than 60Ni, the traditional material for heating elements. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance, corrosion resistance, and surface qualities as well as forming and heat treating. Filing Code: SS-1366. Producer or source: VDM Metals GmbH.
Journal Articles
ATLAS 316, ATLAS 316L, ATLAS 316H: Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2024) 73 (1): SS-1365.
Published: 01 March 2024
Abstract
View articletitled, ATLAS 316, ATLAS 316L, ATLAS 316H: Austenitic Stainless Steel
View
PDF
for article titled, ATLAS 316, ATLAS 316L, ATLAS 316H: Austenitic Stainless Steel
Atlas 316 is a chromium-nickel-molybdenum austenitic stainless steel, second only to Atlas 304 in commercial importance. The molybdenum gives Atlas 316 better overall corrosion resistant properties than type 304 austenitic stainless steel, particularly higher resistance to pitting and crevice corrosion in chloride environments. It is readily brake or roll formed, welded, soldered, and cut by both thermal and mechanical methods. The austenitic structure gives excellent toughness, even down to cryogenic temperatures. Atlas 316L, the low carbon version of Atlas 316, is highly resistant to sensitization (grain boundary carbide precipitation) and so is extensively used in heavy gauge welded components; about 5 mm, 0.2 in., and over. Atlas 316H, with its higher carbon content, has some application at elevated temperatures, as does stabilized type 316Ti. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1365. Producer or source: Atlas Steels.
Journal Articles
SAE 1015, CEN C15, ISO C15: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2024) 73 (1): CS-266.
Published: 01 March 2024
Abstract
View articletitled, SAE 1015, CEN C15, ISO C15: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1015, CEN C15, ISO C15: Wrought Low-Carbon Non-Alloy Steels
1015, C15E, and C15R are wrought low-carbon (carbon equals 0.12 to 0.18 percent) non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-medium strength, excellent cold formability, and excellent weldability are required. These steels may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-266. Producer or source: Heat Treater’s Guide.
Journal Articles
AUSTRAL WRIGHT ALLOY B25 (UNS C17200): Cu-1.9Be Alloy
Available to Purchase
Alloy Digest (2023) 72 (12): Cu-943.
Published: 01 December 2023
Abstract
View articletitled, AUSTRAL WRIGHT ALLOY B25 (UNS C17200): Cu-1.9Be Alloy
View
PDF
for article titled, AUSTRAL WRIGHT ALLOY B25 (UNS C17200): Cu-1.9Be Alloy
Austral Wright Alloy B25 (UNS C17200) is a wrought beryllium copper alloy. It provides the highest strength of any copper alloy, with electrical conductivity considerably greater than that of other high-strength copper alloys. Since it is heat treated after forming, it provides excellent formability and ductility. This alloy features good stress relaxation resistance and high fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-943. Producer or source: Austral Wright Metals.
Journal Articles
SAE 1010, CEN C10, ISO C10: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2023) 72 (12): CS-265.
Published: 01 December 2023
Abstract
View articletitled, SAE 1010, CEN C10, ISO C10: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1010, CEN C10, ISO C10: Wrought Low-Carbon Non-Alloy Steels
1010, C10E, and C10R are wrought low-carbon (carbon = 0.07–0.13%) non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. These steels are characterized by low strength, high ductility, excellent cold formability, and excellent weldability. Within the carbon range of these steel grades, strength and hardness will increase with increase in carbon content and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1010, C10E, and C10R are widely used for lightly stressed parts where cold formability is the primary requisite. They are less expensive than 1008 and can be used when the requirements for cold forming are less exacting. 1010, C10E, and C10R may also be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-265. Producer or source: Heat Treater's Guide.
Journal Articles
MEEHANITE SFP500: Ductile Iron
Available to Purchase
Alloy Digest (2023) 72 (11): CI-108.
Published: 01 November 2023
Abstract
View articletitled, MEEHANITE SFP500: Ductile Iron
View
PDF
for article titled, MEEHANITE SFP500: Ductile Iron
Meehanite SFP500 is a ductile iron that has a minimum tensile strength of 500 MPa (73 ksi) and a minimum elongation of 8%, when measured on test pieces machined from separately cast samples. This Meehanite grade possesses a mixed matrix of ferrite and pearlite, with the ferrite predominating. It offers a compromise between the relatively soft, low tensile, high ductility ferritic types and the harder, higher tensile, lower ductility pearlitic grades. Meehanite SFP500 is a good all-round material providing a degree of toughness coupled with a higher tensile strength in the as-cast condition. This datasheet provides information on physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and heat treating. Filing Code: CI-108. Producer or source: Meehanite Metal Corporation.
Journal Articles
SAE 1008, CEN C8, ISO C8: Wrought Low-Carbon Non-Alloy Steels
Available to Purchase
Alloy Digest (2023) 72 (11): CS-264.
Published: 01 November 2023
Abstract
View articletitled, SAE 1008, CEN C8, ISO C8: Wrought Low-Carbon Non-Alloy Steels
View
PDF
for article titled, SAE 1008, CEN C8, ISO C8: Wrought Low-Carbon Non-Alloy Steels
1008 and C8C are wrought low-carbon (carbon ≤ 0.10%) non-alloy steels that are used in the as-rolled, annealed, normalized, or cold worked condition. These steels are characterized by low strength, high ductility, excellent cold formability, and excellent weldability. Within the carbon range of these steel grades, strength and hardness will increase with increase in carbon content and with cold work. Such increases in strength are at the sacrifice of ductility or the ability to withstand cold deformation. 1008 and C8C are widely used for lightly stressed parts where cold formability or drawability is the primary requirement. In general, they are not intended for heat treatment after cold working.1008 may, however, be used in the case hardened, nitrided, or nitrocarburized condition. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: CS-264. Producer or source: Heat Treater's Guide.
Journal Articles
AURUBIS CuFe0.1P: Wrought Cu-0.1Fe-0.033P Alloy
Available to Purchase
Alloy Digest (2023) 72 (10): Cu-942.
Published: 01 October 2023
Abstract
View articletitled, AURUBIS CuFe0.1P: Wrought Cu-0.1Fe-0.033P Alloy
View
PDF
for article titled, AURUBIS CuFe0.1P: Wrought Cu-0.1Fe-0.033P Alloy
Aurubis CuFe0.1P is a low-alloyed, age hardened copper alloy. It combines very high electrical conductivity (≥ 84% IACS) and thermal conductivity with relatively high strength. The alloy has improved temperature resistance as well as good relaxation properties and is suited for welding and soldering. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance. Filing Code: Cu-942. Producer or source: Aurubis AG.
Journal Articles
MEEHANITE SF450.15: Ferritic Ductile Iron
Available to Purchase
Alloy Digest (2023) 72 (10): CI-107.
Published: 01 October 2023
Abstract
View articletitled, MEEHANITE SF450.15: Ferritic Ductile Iron
View
PDF
for article titled, MEEHANITE SF450.15: Ferritic Ductile Iron
Meehanite SF450.15 is a ductile iron that has a minimum tensile strength of 450 MPa (65 ksi) and a minimum elongation of 15%, when measured on test pieces machined from separately cast samples. This Meehanite grade possesses a predominantly ferritic matrix giving the material a good level of ductility. It is used where a degree of shock resistance at ambient temperatures is important. Meehanite SF450.15 is of particular interest to design engineers wishing to replace fabrications or non-alloy steel castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and heat treating. Filing Code: CI-107. Producer or source: Meehanite Metal Corporation.