Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 4573
Machinability
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (2024) 73 (3): Cu-944.
Published: 01 September 2024
Abstract
View article
PDF
Austral Wright C26000 (70-30 Brass) is a copper-zinc alloy. It has the distinctive clear bright yellow color normally associated with brass. Austral Wright C26000 possesses an excellent combination of strength and ductility. This grade is the most widely available copper alloy in the sheet form. It is often used where its deep drawing qualities are needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-944. Producer or source: Austral Wright Metals.
Journal Articles
Alloy Digest (2024) 73 (2): CI-109.
Published: 01 June 2024
Abstract
View article
PDF
ACO Eurobar EN-GJS-400-18C-LT is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 18%. It has a tensile strength exceeding that of the highest-tensile-strength grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance as well as casting, heat treating, and machining. Filing Code: CI-109. Producer or source: ACO Eurobar GmbH.
Journal Articles
Alloy Digest (2024) 73 (1): SS-1365.
Published: 01 March 2024
Abstract
View article
PDF
Atlas 316 is a chromium-nickel-molybdenum austenitic stainless steel, second only to Atlas 304 in commercial importance. The molybdenum gives Atlas 316 better overall corrosion resistant properties than type 304 austenitic stainless steel, particularly higher resistance to pitting and crevice corrosion in chloride environments. It is readily brake or roll formed, welded, soldered, and cut by both thermal and mechanical methods. The austenitic structure gives excellent toughness, even down to cryogenic temperatures. Atlas 316L, the low carbon version of Atlas 316, is highly resistant to sensitization (grain boundary carbide precipitation) and so is extensively used in heavy gauge welded components; about 5 mm, 0.2 in., and over. Atlas 316H, with its higher carbon content, has some application at elevated temperatures, as does stabilized type 316Ti. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1365. Producer or source: Atlas Steels.
Journal Articles
Alloy Digest (2023) 72 (10): SS-1364.
Published: 01 October 2023
Abstract
View article
PDF
VDM 330 (Nicrofer 3718) is an austenitic iron-nickel-chromium-silicon alloy with good high-temperature strength and good resistance to carburization, thermal shock, and high temperature oxidation. It is used extensively in high-temperature environments where resistance to the combined effects of thermal cycling and carburization is required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1364. Producer or source: VDM Metals GmbH (a subsidiary of Acerinox, S.A.).
Journal Articles
Alloy Digest (2023) 72 (9): Ni-786.
Published: 01 September 2023
Abstract
View article
PDF
VDM 33 (Nicrofer 3033) is an austenitic alloy that has an excellent resistance against common corrosion and pitting corrosion in media containing chloride due to its well-balanced analysis and extraordinarily high chromium content. Also because of its very high strength and good workability, VDM 33 is a material that can be used for many applications in the chemical processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-786. Producer or source: VDM Metals GmbH (a subsidiary of Acerinox, S.A.).
Journal Articles
Alloy Digest (2023) 72 (8): SS-1361.
Published: 01 August 2023
Abstract
View article
PDF
ATI 303 is a free-machining stainless steel specifically designed to exhibit improved machinability. It is the free-machining modification of the basic 18% chromium-8% nickel stainless steel. Sulfur is added to produce the free-machining characteristics. The good mechanical and corrosion-resistant properties of the lower-sulfur grade are retained to the extent possible. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1361. Producer or source: ATI.
Journal Articles
Alloy Digest (2023) 72 (7): Al-500.
Published: 01 July 2023
Abstract
View article
PDF
Raffmetal EN AB-Al Si9Mg (EN AB-43300) is a heat-treatable, aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring a combination of excellent casting characteristics, high strength with excellent ductility, and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, and machining. Filing Code: Al-500. Producer or source: Raffmetal S.p.A.
Journal Articles
Alloy Digest (2023) 72 (7): Ti-194.
Published: 01 July 2023
Abstract
View article
PDF
Elgiloy CP Titanium Grade 2 (Ti 40) is an unalloyed commercially pure titanium. It is widely used for applications requiring a combination of moderate strength, high ductility, excellent corrosion resistance, and good weldability. This grade can be used in the temperature range –184 to 540 °C (–300 to 1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-194. Producer or source: Elgiloy Specialty Metals.
Journal Articles
Alloy Digest (2023) 72 (6): Al-499.
Published: 01 June 2023
Abstract
View article
PDF
Rio Tinto A356.2 is a heat-treatable, aluminum-silicon-magnesium casting alloy (3xx.x series) that is available in the ingot form for remelting. It is used extensively for producing general-purpose sand and permanent mold castings that require a combination of medium strength with good elongation, very good corrosion resistance, and excellent casting characteristics. Alloy A356.0, which is a higher purity, low iron version of alloy 356.0, provides better elongation and somewhat higher tensile strength. Alloy A356.0 is used in premium, higher strength applications and is used extensively in safety critical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-499. Producer or source: Rio Tinto Limited.
Journal Articles
Alloy Digest (2023) 72 (6): Ti-193.
Published: 01 June 2023
Abstract
View article
PDF
Elgiloy CP Titanium Grade 1 / Ti 25 is an unalloyed commercially pure titanium. It has the highest purity, lowest strength, and best ductility and formability of the four ASTM unalloyed titanium grades. This grade can be used in the temperature range -184 to 540 °C (-300 to 1000 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-193. Producer or source: Elgiloy Specialty Metals.
Journal Articles
Alloy Digest (2023) 72 (5): Al-498.
Published: 01 May 2023
Abstract
View article
PDF
Rio Tinto 356.2 is a heat-treatable aluminum-silicon-magnesium casting alloy (3xx.x series) that is available in the ingot form for remelting. It is used extensively for producing general purpose sand and permanent mold castings that require a combination of medium strength, very good corrosion resistance, and excellent casting characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-498. Producer or source: Rio Tinto Limited.
Journal Articles
Alloy Digest (2023) 72 (5): Ti-192.
Published: 01 May 2023
Abstract
View article
PDF
Aubert & Duval TA6V ELI (UNS R56401) is an alpha-beta, titanium-aluminum-vanadium alloy that is normally used in the annealed condition. It is a purer version of Aubert & Duval TA6V, with a lower oxygen and iron content. Aubert & Duval TA6V ELI is especially popular due to its ductility at cryogenic temperatures and its excellent biocompatibility with the human body. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-192. Producer or source: Aubert & Duval S.A.
Journal Articles
Alloy Digest (2023) 72 (5): Ni-782.
Published: 01 May 2023
Abstract
View article
PDF
Aubert & Duval AD730 (NiCr16Co9Mo3W3Ti3Al2 alloy) is a cast and wrought nickel-based superalloy that withstands high temperatures (up to 750 °C, or 1380 °F) while preserving strength, creep, and fatigue resistance at a competitive cost. The breakthroughmainly comes from its unique properties-versus-cost balance, due to its recycling and forging ability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-782. Producer or source: Aubert & Duval S.A.
Journal Articles
Alloy Digest (2023) 72 (4): Ti-191.
Published: 01 April 2023
Abstract
View article
PDF
Aubert & Duval TA6V (UNS R56400) is an alpha–beta, titanium-aluminum-vanadium alloy that is used in the annealed or the solution heat treated and aged condition. It is characterized by high specific strength and excellent corrosion resistance, and is one of the most commonly used titanium alloys. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-191. Producer or source: Aubert & Duval S.A.
Journal Articles
Alloy Digest (2023) 72 (4): Cu-940.
Published: 01 April 2023
Abstract
View article
PDF
L. Klein Declafor 1015 is a ternary copper-nickel-tin spinodal alloy that combines high strength with excellent corrosion resistance and fair machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Cu-940. Producer or source: L. Klein SA.
Journal Articles
Alloy Digest (2023) 72 (4): Al-497.
Published: 01 April 2023
Abstract
View article
PDF
BSI LM2 is an aluminum-silicon-copper casting alloy (3xx.x series). It is essentially a pressure die casting alloy with excellent casting characteristics. Castings made from BSI LM2 have a higher tensile strength and better machinability than pressure die castings made from either BSI LM6 or BSI LM20. The use of BSI LM2 is not recommended for corrosive environments unless protection of the casting by a process such as anodizing is used. It is better in such circumstances to consider the use of either BSI LM6 or BSI LM20. BSI LM2 has a slightly lower density than BSI LM24. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-497. Producer or source: British Standards Institution.
Journal Articles
Alloy Digest (2023) 72 (4): CS-244.
Published: 01 April 2023
Abstract
View article
PDF
1078 and C80S are wrought high-carbon (carbon = 0.72–0.85%) non-alloy steels that are used in the cold worked, quenched and tempered, or austempered condition. These steels are widely used for highly stressed parts, such as springs, that require higher strength levels than can be achieved by the lower carbon grades. They are also used for applications where the higher carbon is needed to improve wear characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-244. Producer or source: Data Survey.
Journal Articles
Alloy Digest (2023) 72 (4): CS-245.
Published: 01 April 2023
Abstract
View article
PDF
1080 is a wrought high-carbon (carbon = 0.75–0.88%) non-alloy steel that is used in the cold worked, quenched and tempered, or austempered condition. This steel is widely used for highly stressed parts, such as springs, that require higher strength levels than can be achieved by the lower carbon grades. It is also used for applications where the higher carbon is needed to improve wear characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-245. Producer or source: Data Survey.
Journal Articles
Alloy Digest (2023) 72 (4): SS-1357.
Published: 01 April 2023
Abstract
View article
PDF
Uddeholm RoyAlloy is a is a patented free machining stainless holder steel that is supplied in the prehardened condition. It is the preferred steel of choice of many mold makers and end users. The steel provides enhanced machinability, improved dimensional stability, and superior surface finish as compared with AISI 420F and X33CrS16 (1.2085) type of steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1357. Producer or source: Uddeholms AB (a voestalpine company).
Journal Articles
Alloy Digest (2023) 72 (3): Ti-190.
Published: 01 March 2023
Abstract
View article
PDF
ATI 8-1-1 (UNS R54810) is a near-alpha alloy with aluminum being the alpha stabilizer, and the additions of molybdenum, vanadium, and iron resulting in small amounts of beta. This alloy is used in the annealed condition, and special duplex annealing procedures have been developed for thick sections such as bars and forgings. It is intended primarily for use at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-190. Producer or source: ATI.