Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 43
Zinc alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1992) 41 (2): Zn-2.
Published: 01 February 1992
Abstract
View article
PDF
ZAMAK-5 has moderately greater hardness, strength and creep resistance than the most widely used general purpose zinc die casting alloy, ZAMAK 3 (See Alloy Digest Zn-1, September 1991). This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Zn-2. Producer or source: Noranda Sales Corporation. Originally published as Zamak-5, May 1954, revised February 1992.
Journal Articles
Alloy Digest (1991) 40 (10): Zn-35.
Published: 01 October 1991
Abstract
View article
PDF
ZA-8 is a zinc-base foundry alloy capable of being sand, permanent mold gravity or die cast (hot-chamber machine). ZA-8 should be the first choice when considering die casting the ZA family (3 alloys) due to its cost effective hot-chamber castability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Zn-35. Producer or source: Noranda Sales Corporation. Originally published November 1980, revised October 1991. See also Zn-48, January 1990.
Journal Articles
Alloy Digest (1991) 40 (9): Zn-1.
Published: 01 September 1991
Abstract
View article
PDF
ZAMAK 3 is the most widely used general purpose zinc-base die casting alloy. It provides an excellent combination of strength and ductility. It has good impact strength. It is the designer's first choice for die casting applications. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Zn-1. Producer or source: Noranda Sales Corporation. Originally published December 1953, revised August 1966, revised September 1991.
Journal Articles
Alloy Digest (1991) 40 (8): Zn-51.
Published: 01 August 1991
Abstract
View article
PDF
ZAMAK 2 is the strongest and hardest of the four Zamak alloys. While generally produced by die casting, ZAMAK 2 is occasionally gravity cast. It is not a widely used alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Zn-51. Producer or source: Noranda Sales Corporation.
Journal Articles
Alloy Digest (1990) 39 (6): Zn-50.
Published: 01 June 1990
Abstract
View article
PDF
ZA-27 is the strongest, hardest and lightest of the three-member ZA alloy group (see also ZA-8, Alloy Digest Zn-48, January 1990, and ZA-12, Alloy Digest Zn-49, May 1990). Mechanical properties of ZA-27 compare favorably with many heavier more costly (manufacturing intensive) alloys such as malleable and ductile iron, manganese and aluminum bronzes and many ferrous and nonferrous wrought alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, forming, machining, and surface treatment. Filing Code: Zn-50. Producer or source: Aluminum Smelting and Refining Company Inc.. See also Alloy Digest Zn-32, October 1977.
Journal Articles
Alloy Digest (1990) 39 (5): Zn-49.
Published: 01 May 1990
Abstract
View article
PDF
ZA-12 is the intermediate member of the family of three ZA die-casting alloys. Its melting point, solidification range and recommended casting-temperature range are greater than those of ZA-8. (See Alloy Digest Zn-48, January 1990). Due to these factors, ZA-12 must be die cast in cold chamber die-casting machines like conventional aluminum die-casting alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, machining, and surface treatment. Filing Code: Zn-49. Producer or source: Aluminum Smelting and Refining Company Inc.. See also Alloy Digest Zn-31, September 1977.
Journal Articles
Alloy Digest (1990) 39 (1): Zn-48.
Published: 01 January 1990
Abstract
View article
PDF
ZA-8 is a hypereutectic zinc-aluminum,highperformance die casting alloy. It is one of a family of three ZA Alloys which can be economically die cast with properties surpassing conventional zinc or aluminum alloys. It is the lowest aluminum content alloy of the family and it has the lowest melting point and casting temperature range. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, machining, and surface treatment. Filing Code: Zn-48. Producer or source: Aluminum Smelting and Refining Company Inc.. See also Alloy Digest Zn-35, revised October 1991.
Journal Articles
Alloy Digest (1989) 38 (3): Zn-47.
Published: 01 March 1989
Abstract
View article
PDF
UNS No. Z33522 is a zinc die casting alloy having superior castability. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Zn-47. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1989) 38 (2): Zn-46.
Published: 01 February 1989
Abstract
View article
PDF
UNS No. Z33531 is a zinc-base alloy containing about 4% aluminum and 1% copper. It is primarily a die casting alloy, having somewhat higher strength than UNS Z33521. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Zn-46. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1988) 37 (12): Zn-45.
Published: 01 December 1988
Abstract
View article
PDF
UNS Z33520 is a zinc-base alloy containing about 4% aluminum. It has no intentionally added copper. It is a relatively ductile (bendable and shapable) die casting alloy. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Zn-45. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1988) 37 (11): Zn-44.
Published: 01 November 1988
Abstract
View article
PDF
UNS No. Z35840 is a zinc-aluminum-copper alloy that offers exceptionally high strength (58,000 to 64,000 psi tensile strength as cast) at modest cost. It performs best in thin-walled castings (down to 0.10 inch) which means reduced weight and lower material costs when castings are redesigned. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion and wear resistance as well as forming, heat treating, machining, and surface treatment. Filing Code: Zn-44. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1988) 37 (7): Zn-43.
Published: 01 July 1988
Abstract
View article
PDF
UNS No. Z35630 is a zinc-aluminum-copper foundry alloy recommended for general-purpose castings of high strength at moderate cost. It was designed for use in nonferrous foundries to compete with cast-iron, bronze, brass and aluminum castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion and wear resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-43. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1988) 37 (3): Zn-42.
Published: 01 March 1988
Abstract
View article
PDF
UNS No. Z35635 is a zinc-aluminum-copper-magnesium foundry alloy recommended for castings of moderate strength and low cost. It was designed for use in nonferrous permanent-mold foundries to compete with cast-iron, aluminum and bronze castings. The alloy can be sand cast and die cast. Its many uses include hardware, valves, implement components and equipment for liquid fuel transfer because it is non-sparking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion and wear resistance as well as casting, heat treating, machining, and surface treatment. Filing Code: Zn-42. Producer or source: Zinc alloy producers.
Journal Articles
Alloy Digest (1987) 36 (6): Zn-41.
Published: 01 June 1987
Abstract
View article
PDF
WEIRKOTE PLUS is a Galfan-coated sheet steel. The sheet is conventional low-carbon steel normally used for galvanized sheets and strip. This digest will concentrate on the characteristics and properties of the Galfan coating which is nominally a 95% zinc-5% aluminum alloy. The coating on Weirkote Plus is ideal for a variety of tough applications. It is excellent for products that require deep drawing and it combines extra corrosion resistance with superior formability. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, joining, and surface treatment. Filing Code: Zn-41. Producer or source: Weirton Steel Corp.
Journal Articles
Alloy Digest (1984) 33 (4): Zn-40.
Published: 01 April 1984
Abstract
View article
PDF
GALFAN is a zinc-5% aluminum alloy with an addition of mischmetal to introduce small amounts of the rare-earth elements lanthanum and cerium. Its composition is eutectic and it was developed to provide a hot-dip coating alloy that would be better than zinc as a protective coating for steel. GALFAN can be used to coat steel sheet, strip and wire with only minor modification of the existing equipment used to produce galvanized steel. GALFAN coatings have good performance characteristics in a variety of applications. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: Zn-40. Producer or source: Zinc Research Organization Inc..
Journal Articles
Alloy Digest (1982) 31 (9): Zn-39.
Published: 01 September 1982
Abstract
View article
PDF
KIDD Alloy ZA-27 is a zinc-aluminum-copper high-strength foundry alloy. It is well suited to structural applications, once the exclusive domain of malleable cast iron, bronzes and aluminum. ZA-27 offers an as-sand-cast tensile strength of 58,000 to 64,000 psi at modest cost; also, it can be cast in cold-chamber machines for better properties than those of conventional die-casting alloys. It is extremely resistant to galling because it has natural lubricity and is thus well suited to bearing and bushing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-39. Producer or source: Kidd Creek Mines Ltd.
Journal Articles
Alloy Digest (1982) 31 (8): Zn-38.
Published: 01 August 1982
Abstract
View article
PDF
KIDD Alloy ZA-12 is the general-purpose, zinc-aluminum-copper foundry alloy. It can be sand, permanent-mold or die cast. Alloy ZA-12 has a modest cost and a tensile strength suitable for many applications where bronze and cast or malleable iron were traditionally used. Alloy ZA-12 is extremely resistant to galling, has natural lubricity and is thus well suited to lubricated bearing and bushing applications. It is particularly well suited to liquid and gas-pressure applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-38. Producer or source: Kidd Creek Mines Ltd.
Journal Articles
Alloy Digest (1981) 30 (8): Zn-37.
Published: 01 August 1981
Abstract
View article
PDF
Tg-12 Zinc Alloy is the general-purpose, zinc-aluminum-copper foundry alloy. It can be sand, permanent-mold or die cast, has a modest cost and a tensile strength suitable for many applications where bronze and cast or malleable iron were traditionally used. Tg-12 is extremely resistant to galling, has natural lubricity and is thus well suited to lubricated bearing and bushing applications. Tg-12 is particularly well suited to liquid and gas-pressure applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-37. Producer or source: Texasgulf Inc..
Journal Articles
Alloy Digest (1981) 30 (6): Zn-36.
Published: 01 June 1981
Abstract
View article
PDF
Tg 27 Zinc Alloy is a zinc-aluminum-copper high-strength foundry alloy that is well suited to structural applications, once the exclusive domain of malleable and cast iron, bronzes and aluminum. Tg 27 offers an as-sand-cast tensile strength of 58,000 to 64,000 psi at modest costs. It is extremely resistant to galling because it has natural lubricity and is thus well suited to bearing and bushing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and surface treatment. Filing Code: Zn-36. Producer or source: Texasgulf Inc..
Journal Articles
Alloy Digest (1978) 27 (10): Zn-34.
Published: 01 October 1978
Abstract
View article
PDF
SUPER-Z is a superplastic zinc-aluminum alloy basically of the eutectoid composition of 78% zinc-22% aluminum with various minor additives to improve its properties, such as strength and creep resistance. Four grades of superplastic zinc alloys are available: SUPER-Z 100, SUPER-Z 200, SUPER-Z 300 and SUPER-Z 400. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zn-34. Producer or source: The New Jersey Zinc Company.