Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 774
Nickel alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
AUBERT & DUVAL PER72: Nickel-Base Superalloy
Available to Purchase
Alloy Digest (2024) 73 (3): Ni-787.
Published: 01 September 2024
Abstract
View articletitled, AUBERT & DUVAL PER72: Nickel-Base Superalloy
View
PDF
for article titled, AUBERT & DUVAL PER72: Nickel-Base Superalloy
Aubert and Duval PER72 (NiCr18Co15TiMoAI alloy) is a precipitation hardening, nickel-base superalloy. The alloy is solid solution strengthened by additions of chromium, cobalt, molybdenum, and tungsten, while additions of titanium and aluminum provide precipitation strengthening. Aubert & Duval PER72 combines high strength with metallurgical stability as demonstrated by excellent impact strength retention after long exposures at elevated temperatures. It also exhibits good oxidation resistance, as well as excellent resistance to sulfide corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on low temperature performance, high temperature performance, and corrosion resistance as well as forming and heat treating. Filing Code: Ni-787. Producer or source: Aubert & Duval S.A. (a member of the Eramet Group).
Journal Articles
VDM 33: High-Chromium Austenitic Alloy
Available to Purchase
Alloy Digest (2023) 72 (9): Ni-786.
Published: 01 September 2023
Abstract
View articletitled, VDM 33: High-Chromium Austenitic Alloy
View
PDF
for article titled, VDM 33: High-Chromium Austenitic Alloy
VDM 33 (Nicrofer 3033) is an austenitic alloy that has an excellent resistance against common corrosion and pitting corrosion in media containing chloride due to its well-balanced analysis and extraordinarily high chromium content. Also because of its very high strength and good workability, VDM 33 is a material that can be used for many applications in the chemical processing industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-786. Producer or source: VDM Metals GmbH (a subsidiary of Acerinox, S.A.).
Journal Articles
BÖHLER L306 VMR: Wrought Ni-Cr-Ti-Al Alloy
Available to Purchase
Alloy Digest (2023) 72 (8): Ni-785.
Published: 01 August 2023
Abstract
View articletitled, BÖHLER L306 VMR: Wrought Ni-Cr-Ti-Al Alloy
View
PDF
for article titled, BÖHLER L306 VMR: Wrought Ni-Cr-Ti-Al Alloy
Böhler L306 VMR is a wrought, age-hardenable nickel-chromium alloy, strengthened by additions of titanium, aluminum, and carbon. It has been developed as a creep-resisting alloy for service at temperatures up to 815 °C (1500 °F). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: Ni-785. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.
Journal Articles
BÖHLER L090: Wrought Ni-Cr-Co-Ti-Al Alloy
Available to Purchase
Alloy Digest (2023) 72 (7): Ni-784.
Published: 01 July 2023
Abstract
View articletitled, BÖHLER L090: Wrought Ni-Cr-Co-Ti-Al Alloy
View
PDF
for article titled, BÖHLER L090: Wrought Ni-Cr-Co-Ti-Al Alloy
Böhler L090 is a wrought, precipitation-hardenable, nickel-chromium-cobalt alloy that is strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 900 °C (1650 °F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: Ni-784. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.
Journal Articles
AUBERT & DUVAL NY690: Nickel-Based Superalloy
Available to Purchase
Alloy Digest (2023) 72 (6): Ni-783.
Published: 01 June 2023
Abstract
View articletitled, AUBERT & DUVAL NY690: Nickel-Based Superalloy
View
PDF
for article titled, AUBERT & DUVAL NY690: Nickel-Based Superalloy
Aubert & Duval NY690 (NiCr30Fe alloy) is a high-chromium nickel alloy that has excellent resistance to many corrosive aqueous media and high temperature atmospheres. In addition to its corrosion resistance, Aubert & Duval NY690 has high strength, good metallurgical stability, and favorable fabrication characteristics. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and heat treating. Filing Code: Ni-783. Producer or source: Aubert & Duval S.A.
Journal Articles
AUBERT & DUVAL AD730: Nickel-Based Superalloy
Available to Purchase
Alloy Digest (2023) 72 (5): Ni-782.
Published: 01 May 2023
Abstract
View articletitled, AUBERT & DUVAL AD730: Nickel-Based Superalloy
View
PDF
for article titled, AUBERT & DUVAL AD730: Nickel-Based Superalloy
Aubert & Duval AD730 (NiCr16Co9Mo3W3Ti3Al2 alloy) is a cast and wrought nickel-based superalloy that withstands high temperatures (up to 750 °C, or 1380 °F) while preserving strength, creep, and fatigue resistance at a competitive cost. The breakthroughmainly comes from its unique properties-versus-cost balance, due to its recycling and forging ability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-782. Producer or source: Aubert & Duval S.A.
Journal Articles
BÖHLER L022: Ni-Cr-Mo Alloy
Available to Purchase
Alloy Digest (2022) 71 (9): Ni-781.
Published: 01 September 2022
Abstract
View articletitled, BÖHLER L022: Ni-Cr-Mo Alloy
View
PDF
for article titled, BÖHLER L022: Ni-Cr-Mo Alloy
Böhler L022 is a nickel-chromium-molybdenum alloy that exhibits very good corrosion resistance, for example, outstanding resistance to pitting, crevice corrosion, and stress-corrosion cracking. It has excellent resistance to oxidizing aqueous media including wet chlorine and mixtures containing nitric acid or oxidizing acids with chloride ions. This alloy also has outstanding resistance to reducing aqueous media. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, and joining. Filing Code: Ni-781. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.
Journal Articles
SPS TECHNOLOGIES AEREX 350: Nickel-Based Superalloy
Available to Purchase
Alloy Digest (2022) 71 (6): Ni-780.
Published: 01 June 2022
Abstract
View articletitled, SPS TECHNOLOGIES AEREX 350: Nickel-Based Superalloy
View
PDF
for article titled, SPS TECHNOLOGIES AEREX 350: Nickel-Based Superalloy
SPS Technologies Aerex 350 is a proprietary high-strength, corrosion-resistant nickel-based superalloy that is suitable for demanding applications up to 730 °C (1350 °F). It has the highest temperature limit of the three SPS superalloys. Like MP35N and MP159, this alloy not only undergoes the multiphase reaction, but also benefits from two additional strengthening mechanisms. Elements are also added to the chemical composition to cause precipitation of the gamma prime phase with higher temperature capability than MP159. Because this alloy is used at even higher temperatures than MP159, elements are added to the chemical composition to also cause the precipitation of eta phase during thermal treatments. This phase contributes to notch toughness at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance. Filing Code: Ni-780. Producer or source: SPS Technologies, Inc.
Journal Articles
BÖHLER L080A: Ni-Cr-Ti-Al Alloy
Available to Purchase
Alloy Digest (2022) 71 (4): Ni-779.
Published: 01 April 2022
Abstract
View articletitled, BÖHLER L080A: Ni-Cr-Ti-Al Alloy
View
PDF
for article titled, BÖHLER L080A: Ni-Cr-Ti-Al Alloy
Böhler L080A is a wrought, precipitation-hardenable, nickel-chromium-titanium-aluminum alloy that is creep resistant up to 850 °C (1560 °F) and has excellent oxidation resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming and heat treating. Filing Code: Ni-779. Producer or source: voestalpine Böhler Edelstahl GmbH & Co KG.
Journal Articles
VDM NICKEL 200: Ni99.2
Available to Purchase
Alloy Digest (2021) 70 (12): Ni-778.
Published: 01 December 2021
Abstract
View articletitled, VDM NICKEL 200: Ni99.2
View
PDF
for article titled, VDM NICKEL 200: Ni99.2
VDM Nickel 200 is an unalloyed nickel grade that contains at least 99.2% nickel. It has characteristics that are useful in several fields, notably chemical processing and electronics. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-778. Producer or source: VDM Metals GmbH (a subsidiary of Acerinox, S.A.).
Journal Articles
CARTECH 617: Ni-22Cr-12.5Co-9Mo Alloy
Available to Purchase
Alloy Digest (2021) 70 (11): Ni-777.
Published: 01 November 2021
Abstract
View articletitled, CARTECH 617: Ni-22Cr-12.5Co-9Mo Alloy
View
PDF
for article titled, CARTECH 617: Ni-22Cr-12.5Co-9Mo Alloy
CarTech 617 (Pyromet 617) is a corrosion and oxidation-resistant, high-temperature nickel-chromium-cobalt-molybdenum alloy. It is solid-solution strengthened with cobalt and molybdenum. Oxidation resistance is imparted through the addition of chromium and aluminum. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-777. Producer or source: Carpenter Technology Corporation.
Journal Articles
ATI X-751: Nickel-Base Superalloy
Available to Purchase
Alloy Digest (2021) 70 (10): Ni-776.
Published: 01 October 2021
Abstract
View articletitled, ATI X-751: Nickel-Base Superalloy
View
PDF
for article titled, ATI X-751: Nickel-Base Superalloy
ATI X-751 is a high-aluminum version of ATI X-750. It is a high-strength, precipitation hardenable, nickel-chromium alloy that employs nickel and titanium as the hardening elements. The alloy has good creep-rupture strength up to 815 °C (1500 °F), and excellent oxidation and corrosion resistance up to 980 °C (1800 °F). This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-776. Producer or source: ATI.
Journal Articles
VDM 36: 64Fe-36Ni Alloy
Available to Purchase
Alloy Digest (2021) 70 (9): Ni-775.
Published: 01 September 2021
Abstract
View articletitled, VDM 36: 64Fe-36Ni Alloy
View
PDF
for article titled, VDM 36: 64Fe-36Ni Alloy
VDM 36 (Pernifer 36) is a binary iron-nickel alloy with a particularly low coefficient of linear thermal expansion. This alloy is used for applications where dimensional changes due to temperature variation must be minimized or in conjunction with high expansion alloys in applications where a motion is desired when the temperature changes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-775. Producer or source: VDM Metals GmbH.
Journal Articles
SPECIAL METALS INCONEL G-3: Ni-22.25Cr-19.5Fe-7Mo-2Cu Alloy
Available to Purchase
Alloy Digest (2021) 70 (8): Ni-774.
Published: 01 August 2021
Abstract
View articletitled, SPECIAL METALS INCONEL G-3: Ni-22.25Cr-19.5Fe-7Mo-2Cu Alloy
View
PDF
for article titled, SPECIAL METALS INCONEL G-3: Ni-22.25Cr-19.5Fe-7Mo-2Cu Alloy
Special Metals Inconel G-3 is a nickel-chromium-iron alloy with additions of molybdenum and copper. Some of the minor elements are controlled to yield increased resistance to heat affected-zone (HAZ) corrosion and improved weldability. Special Metals Inconel G-3 has excellent corrosion resistance to oxidizing chemicals and atmospheres. It is also resistant to reducing chemicals because of its nickel and copper contents. The nickel content also provides the alloy with exceptional stress-corrosion-cracking resistance in chloride-containing environments. The high molybdenum content provides very good resistance to pitting and crevice corrosion. The low carbon content helps prevent sensitization, giving the alloy resistance to intergranular corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-774. Producer or source: Special Metals Corporation.
Journal Articles
NIPPON YAKIN NAS 800: Ni-Fe-Cr Alloy
Available to Purchase
Alloy Digest (2021) 70 (7): Ni-773.
Published: 01 July 2021
Abstract
View articletitled, NIPPON YAKIN NAS 800: Ni-Fe-Cr Alloy
View
PDF
for article titled, NIPPON YAKIN NAS 800: Ni-Fe-Cr Alloy
Nippon Yakin NAS 800 is an austenitic nickel-iron-chromium alloy that exhibits high strength and excellent resistance to oxidation and carburization at high temperatures. It also offers excellent corrosion resistance in many aqueous environments. It is normally employed in service temperatures up to and including 600 °C (1100 °F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Ni-773. Producer or source: Nippon Yakin Kogyo Co., Ltd.
Journal Articles
ATI 690: Ni-30Cr-10Fe Alloy
Available to Purchase
Alloy Digest (2021) 70 (6): Ni-771.
Published: 01 June 2021
Abstract
View articletitled, ATI 690: Ni-30Cr-10Fe Alloy
View
PDF
for article titled, ATI 690: Ni-30Cr-10Fe Alloy
ATI 690 is a nickel-chromium-iron alloy that is intended for the production of nuclear grade tube that meets the requirements outlined in ATI 690 Alloy TREX, ATI, 2012. This alloy exhibits excellent resistance to many corrosive aqueous media and high temperature atmospheres. In addition to its corrosion resistance, ATI 690 has high strength, good metallurgical stability, and favorable fabrication characteristics. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-771. Producer or source: ATI.
Journal Articles
VDM HT 80: Ni-20Cr-1.25Si Alloy
Available to Purchase
Alloy Digest (2021) 70 (6): Ni-772.
Published: 01 June 2021
Abstract
View articletitled, VDM HT 80: Ni-20Cr-1.25Si Alloy
View
PDF
for article titled, VDM HT 80: Ni-20Cr-1.25Si Alloy
VDM HT 80 is an austenitic, Ni-20Cr-1.25Si alloy that is typically used for the manufacture of resistors and heating conductors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: Ni-772. Producer or source: VDM Metals GmbH.
Journal Articles
NIPPON YAKIN NAS H330: Ni-Fe-Cr-Si Alloy
Available to Purchase
Alloy Digest (2021) 70 (5): Ni-770.
Published: 01 May 2021
Abstract
View articletitled, NIPPON YAKIN NAS H330: Ni-Fe-Cr-Si Alloy
View
PDF
for article titled, NIPPON YAKIN NAS H330: Ni-Fe-Cr-Si Alloy
Nippon Yakin NAS H330 (UNS N08330) is an austenitic nickel-iron-chromium-silicon alloy that combines excellent high temperature strength, metallurgical stability, and corrosion resistance, with superior resistance to carburization and nitridation. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Ni-770. Producer or source: Nippon Yakin Kogyo Co., Ltd.
Journal Articles
VDM 601: 60Ni-23Cr-15Fe-1.4Al-0.06C Alloy
Available to Purchase
Alloy Digest (2021) 70 (4): Ni-769.
Published: 01 April 2021
Abstract
View articletitled, VDM 601: 60Ni-23Cr-15Fe-1.4Al-0.06C Alloy
View
PDF
for article titled, VDM 601: 60Ni-23Cr-15Fe-1.4Al-0.06C Alloy
VDM 601 (Nicrofer 6023 H) is a nickel-chromium-iron alloy with additions of aluminum and titanium. This alloy is specifically recommended for service above 550 °C (1020 °F) because of its superior creep-rupture properties resulting from its controlled carbon content and coarse grain size. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Ni-769. Producer or source: VDM Metals GmbH.
Journal Articles
SPECIAL METALS INCONEL C-276: Ni-16Mo-15Cr-6Fe-4W Alloy
Available to Purchase
Alloy Digest (2021) 70 (3): Ni-768.
Published: 01 March 2021
Abstract
View articletitled, SPECIAL METALS INCONEL C-276: Ni-16Mo-15Cr-6Fe-4W Alloy
View
PDF
for article titled, SPECIAL METALS INCONEL C-276: Ni-16Mo-15Cr-6Fe-4W Alloy
Special Metals Inconel C-276 is a wrought, Ni-Mo-Cr-Fe-W alloy that has excellent corrosion resistance in a wide range of aggressive media. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain resistance to intergranular attack in heat-affected zones of welded joints. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-768. Producer or source: Special Metals Corporation.
1