Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 83
Magnesium alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
AM60A, AM60B: Magnesium and Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (10): MG-88.
Published: 01 October 2018
Abstract
View articletitled, AM60A, AM60B: Magnesium and Casting Alloy
View
PDF
for article titled, AM60A, AM60B: Magnesium and Casting Alloy
Magnesium AM50A is a die casting alloy and has good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Mg-87. Producer or source: Multiple producers.
Journal Articles
AM50A: Magnesium and Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (9): MG-87.
Published: 01 September 2018
Abstract
View articletitled, AM50A: Magnesium and Casting Alloy
View
PDF
for article titled, AM50A: Magnesium and Casting Alloy
Magnesium AM50A is a die casting alloy and has good strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Mg-87. Producer or source: Multiple producers.
Journal Articles
ZC63A: Magnesium and Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (8): Mg-86.
Published: 01 August 2018
Abstract
View articletitled, ZC63A: Magnesium and Casting Alloy
View
PDF
for article titled, ZC63A: Magnesium and Casting Alloy
Magnesium ZC63A is a sand casting alloy that is heat treatable (T6) and has good strength. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as heat treating. Filing Code: Mg-86. Producer or source: Multiple producers.
Journal Articles
K1A: Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (6): Mg-85.
Published: 01 June 2018
Abstract
View articletitled, K1A: Magnesium Casting Alloy
View
PDF
for article titled, K1A: Magnesium Casting Alloy
Magnesium K1A is the casting alloy with the highest vibration-damping index. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as casting, machining, and joining. Filing Code: Mg-85. Producer or source: Multiple producers.
Journal Articles
EV31A: Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (5): Mg-84.
Published: 01 May 2018
Abstract
View articletitled, EV31A: Magnesium Casting Alloy
View
PDF
for article titled, EV31A: Magnesium Casting Alloy
EV31A is a heat treatable sand and investment casting alloy. It is typically furnished in the T-6 temper. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-84. Producer or source: Multiple producers.
Journal Articles
AZ91E: Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (4): Mg-83.
Published: 01 April 2018
Abstract
View articletitled, AZ91E: Magnesium Casting Alloy
View
PDF
for article titled, AZ91E: Magnesium Casting Alloy
AZ91E is a general-purpose sand and investment casting alloy. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-83. Producer or source: Multiple producers.
Journal Articles
AS41A, AS41B: Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2018) 67 (3): Mg-82.
Published: 01 March 2018
Abstract
View articletitled, AS41A, AS41B: Magnesium Casting Alloy
View
PDF
for article titled, AS41A, AS41B: Magnesium Casting Alloy
AS41A and AS41B are die casting alloys with a good combination of ductility and strength. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as casting and joining. Filing Code: Mg-82. Producer or source: Multiple producers.
Journal Articles
ELEKTRON 675: Extrusion Alloy
Available to Purchase
Alloy Digest (2015) 64 (10): Mg-81.
Published: 01 October 2015
Abstract
View articletitled, ELEKTRON 675: Extrusion Alloy
View
PDF
for article titled, ELEKTRON 675: Extrusion Alloy
Elektron 675 is an extrusion alloy designed for high strength to 250 deg C (482 deg F). This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Mg-81. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON EQ2: General Purpose
Available to Purchase
Alloy Digest (2015) 64 (9): Mg-80.
Published: 01 September 2015
Abstract
View articletitled, ELEKTRON EQ2: General Purpose
View
PDF
for article titled, ELEKTRON EQ2: General Purpose
Elektron EQ21 is a casting high strength magnesium alloy developed as a heat treatable alloy with rare earth element additions. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bend strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, heat treating, machining, joining, and surface treatment. Filing Code: Mg-80. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON AZ91E: General Purpose
Available to Purchase
Alloy Digest (2015) 64 (8): Mg-79.
Published: 01 August 2015
Abstract
View articletitled, ELEKTRON AZ91E: General Purpose
View
PDF
for article titled, ELEKTRON AZ91E: General Purpose
Elektron AZ91E is a sand casting magnesium alloy developed for general purpose applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, forming, heat treating, joining, and surface treatment. Filing Code: Mg-79. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON AZ31B: Heat Treatable Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2011) 60 (10): Mg-78.
Published: 01 October 2011
Abstract
View articletitled, ELEKTRON AZ31B: Heat Treatable Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON AZ31B: Heat Treatable Magnesium Casting Alloy
ELEKTRON AZ31B is a wrought magnesium alloy developed to offer good properties maintaining corrosion resistance and weldability. The alloy is used in aerospace, automotive, and military applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance and surface qualities as well as forming, heat treating, machining, and joining. Filing Code: Mg-78. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON WE54: Heat Treatable Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2009) 58 (4): Mg-77.
Published: 01 April 2009
Abstract
View articletitled, ELEKTRON WE54: Heat Treatable Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON WE54: Heat Treatable Magnesium Casting Alloy
ElektronWE54 is fully heat treatable for use to 300 deg C (570 deg F) and is free of silver and thorium. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-77. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON WE43: Heat Treatable Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2009) 58 (3): Mg-76.
Published: 01 March 2009
Abstract
View articletitled, ELEKTRON WE43: Heat Treatable Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON WE43: Heat Treatable Magnesium Casting Alloy
Elektron WE43 was developed by Magnesium Elektron for use to 300 deg C and has good mechanical properties at these temperatures. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-76. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON 21: Heat Treatable Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2009) 58 (2): Mg-75.
Published: 01 February 2009
Abstract
View articletitled, ELEKTRON 21: Heat Treatable Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON 21: Heat Treatable Magnesium Casting Alloy
ELEKTRON 21 has been developed to offer improved properties and superior corrosion resistance while maintaining the processing advantages of the Mg-Zn-rare earth alloys. The alloy is used in military and motorsport applications where these properties are at a premium. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-75. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
ELEKTRON MSR-B: Heat Treatable Magnesium Casting Alloy
Available to Purchase
Alloy Digest (2009) 58 (1): Mg-74.
Published: 01 January 2009
Abstract
View articletitled, ELEKTRON MSR-B: Heat Treatable Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON MSR-B: Heat Treatable Magnesium Casting Alloy
ELEKTRON Alloy Elektron MSR-B is a magnesium casting alloy developed to offer good properties while retaining good foundry characteristics. The alloy is used in aerospace and military applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: MG-74. Producer or source: Magnesium Elektron Wrought Products, North America.
Journal Articles
KANTHAL 200R10: Thermostatic Bimetal
Available to Purchase
Alloy Digest (2008) 57 (5): Mn-4.
Published: 01 May 2008
Abstract
View articletitled, KANTHAL 200R10: Thermostatic Bimetal
View
PDF
for article titled, KANTHAL 200R10: Thermostatic Bimetal
Kanthal 200R10 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 250 deg C (−4 to 480 deg F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: MN-4. Producer or source: Kanthal AB.
Journal Articles
AZ91D and AZ91E ALLOYS: High Purity Magnesium Aluminum Zinc Manganese Alloys
Available to Purchase
Alloy Digest (1988) 37 (5): Mg-73.
Published: 01 May 1988
Abstract
View articletitled, AZ91D and AZ91E ALLOYS: High Purity Magnesium Aluminum Zinc Manganese Alloys
View
PDF
for article titled, AZ91D and AZ91E ALLOYS: High Purity Magnesium Aluminum Zinc Manganese Alloys
AZ91D and AZ91E alloys are magnesium-aluminum-zinc-manganese alloys of closely controlled purity. Ingot is available for use in the production of improved corrosion resistant sand, permanent-mold and die castings. AZ91D is used for die casting and AZ91E for sand and permanent-mold castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-73. Producer or source: The Dow Chemical Company.
Journal Articles
ELEKTRON QH21A: Casting Alloy for Use at Elevated Temperatures
Available to Purchase
Alloy Digest (1979) 28 (1): Mg-72.
Published: 01 January 1979
Abstract
View articletitled, ELEKTRON QH21A: Casting Alloy for Use at Elevated Temperatures
View
PDF
for article titled, ELEKTRON QH21A: Casting Alloy for Use at Elevated Temperatures
ELEKTRON QH21A is a magnesium-base casting alloy developed to meet the ever increasing requirements for casting alloys to operate at elevated temperatures. It is of particular interest to designers and stress engineers for highly stressed components operating at temperatures up to 480 F (250 C), especially where pressure tightness is a requirement. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Mg-72. Producer or source: Magnesium Elektron Inc..
Journal Articles
ELEKTRON ZE63A: Magnesium Casting Alloy
Available to Purchase
Alloy Digest (1973) 22 (5): Mg-71.
Published: 01 May 1973
Abstract
View articletitled, ELEKTRON ZE63A: Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON ZE63A: Magnesium Casting Alloy
ELEKTRON ZE63A is a high-strength magnesium casting alloy having good foundry characteristics. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-71. Producer or source: Magnesium Elektron Inc..
Journal Articles
ELEKTRON ZE41A: Medium Strength Magnesium Casting Alloy
Available to Purchase
Alloy Digest (1970) 19 (10): Mg-70.
Published: 01 October 1970
Abstract
View articletitled, ELEKTRON ZE41A: Medium Strength Magnesium Casting Alloy
View
PDF
for article titled, ELEKTRON ZE41A: Medium Strength Magnesium Casting Alloy
ELEKTRON ZE41A is a medium-strength, high-integrity magnesium casting alloy which is fully weldable and has good fatigue and creep properties. It has maximum freedom from microporosity and is applicable up to 320 F. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Mg-70. Producer or source: Magnesium Elektron Inc..
1