Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 86
Aluminum bronze
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
CONCAST C95900: Aluminum Bronze
Available to Purchase
Alloy Digest (2019) 68 (12): Cu-902.
Published: 01 December 2019
Abstract
View articletitled, CONCAST C95900: Aluminum Bronze
View
PDF
for article titled, CONCAST C95900: Aluminum Bronze
Concast C95900 is a cast nickel-aluminum-bronze alloy. Aluminum bronze is the highest strength standard copper-based alloy. The nickel content in C95900 enhances its mechanical strength, wear, and corrosion resistance, making it suitable for heavy-duty applications. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating, machining, and joining. Filing Code: Cu-902. Producer or source: Concast Metal Products Co..
Journal Articles
WIELAND-UB6: Aluminum Bronze Alloy
Available to Purchase
Alloy Digest (2019) 68 (12): Cu-888.
Published: 01 December 2019
Abstract
View articletitled, WIELAND-UB6: Aluminum Bronze Alloy
View
PDF
for article titled, WIELAND-UB6: Aluminum Bronze Alloy
Wieland-UB5 is complex aluminum bronze that has excellent machinability, high hardness, and high compressive strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on high temperature performance, corrosion and wear resistance as well as forming, heat treating, and machining. Filing Code: Cu-888. Producer or source: Wieland Metals, Inc.. Originally published May 2019, corrected December 2019.
Journal Articles
Concast C95500: Nickel Aluminum Bronze
Available to Purchase
Alloy Digest (2019) 68 (11): Cu-900.
Published: 01 November 2019
Abstract
View articletitled, Concast C95500: Nickel Aluminum Bronze
View
PDF
for article titled, Concast C95500: Nickel Aluminum Bronze
Concast C95500 is a cast nickel-aluminum bronze alloy. Aluminum bronze is the highest strength standard copper-based alloy. The nickel content in C95500 greatly enhances its mechanical strength, and wear and corrosion resistance, making it suitable for heavyduty applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Cu-900. Producer or source: Concast Metal Products Co..
Journal Articles
CONCAST C95300HT: Aluminum Bronze
Available to Purchase
Alloy Digest (2019) 68 (10): Cu-898.
Published: 01 October 2019
Abstract
View articletitled, CONCAST C95300HT: Aluminum Bronze
View
PDF
for article titled, CONCAST C95300HT: Aluminum Bronze
Concast C95300HT is a high-strength aluminum bronze casting alloy. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as machining. Filing Code: Cu-898. Producer or source: Concast Metal Products Company.
Journal Articles
CONCAST AMS 4880-C95510: Nickel-Aluminum Bronze Casting
Available to Purchase
Alloy Digest (2019) 68 (9): Cu-895.
Published: 01 September 2019
Abstract
View articletitled, CONCAST AMS 4880-C95510: Nickel-Aluminum Bronze Casting
View
PDF
for article titled, CONCAST AMS 4880-C95510: Nickel-Aluminum Bronze Casting
AMS 4880-C95510 is a nickel-aluminum bronze casting useful for bushings and bearings. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining. Filing Code: Cu-895. Producer or source: Concast Metal Products Company.
Journal Articles
WIELAND-UB7: Aluminum Bronze Alloy
Available to Purchase
Alloy Digest (2015) 64 (4): Cu-836.
Published: 01 April 2015
Abstract
View articletitled, WIELAND-UB7: Aluminum Bronze Alloy
View
PDF
for article titled, WIELAND-UB7: Aluminum Bronze Alloy
Wieland-UB7 is an aluminum bronze alloy with high hardness and compressive strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-836. Producer or source: Wieland Metals Inc..
Journal Articles
WIELAND-UB5: Aluminum Bronze Alloy
Available to Purchase
Alloy Digest (2015) 64 (3): Cu-835.
Published: 01 March 2015
Abstract
View articletitled, WIELAND-UB5: Aluminum Bronze Alloy
View
PDF
for article titled, WIELAND-UB5: Aluminum Bronze Alloy
Wieland-UB5 is an aluminum bronze alloy with good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-835. Producer or source: Wieland Metals Inc..
Journal Articles
ANSONIA ALLOY C64200 and C64210: Aluminum Bronze Alloys
Available to Purchase
Alloy Digest (2013) 62 (3): Cu-816.
Published: 01 March 2013
Abstract
View articletitled, ANSONIA ALLOY C64200 and C64210: Aluminum Bronze Alloys
View
PDF
for article titled, ANSONIA ALLOY C64200 and C64210: Aluminum Bronze Alloys
Ansonia alloys C64200 and C64210 are aluminum bronze alloys with great machinability for alloys without lead. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-816. Producer or source: Ansonia Copper & Brass Inc..
Journal Articles
ELECTRALLOY EC63000/EC63200: Nickel-Aluminum-Bronze Alloy
Available to Purchase
Alloy Digest (2009) 58 (12): Cu-776.
Published: 01 December 2009
Abstract
View articletitled, ELECTRALLOY EC63000/EC63200: Nickel-Aluminum-Bronze Alloy
View
PDF
for article titled, ELECTRALLOY EC63000/EC63200: Nickel-Aluminum-Bronze Alloy
ELECTRALLOY EC63000 and EC63200 are age-hardenable nickel-aluminum-bronze alloys with strength and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-776. Producer or source: Electralloy, a Division of G.O. Carlson Inc.
Journal Articles
HIDURAX 1: Nickel Molybdenum Case Hardening Steel
Available to Purchase
Alloy Digest (2006) 55 (2): Cu-740.
Published: 01 February 2006
Abstract
View articletitled, HIDURAX 1: Nickel Molybdenum Case Hardening Steel
View
PDF
for article titled, HIDURAX 1: Nickel Molybdenum Case Hardening Steel
Hidurax 1 is a complex nickel-aluminum bronze possessing good mechanical strength and hardness. Advantages and benefits to be obtained with this alloy include ductility, corrosion resistance, wear resistance, superior bearing properties, and fatigue strength. The excellent properties of Hidurax 1 are maintained at elevated temperatures, and the alloy possesses very good resistance to oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: CU-740. Producer or source: Langley Alloys.
Journal Articles
MOLDSTAR 18, 21, 22: Aluminum Bronze Alloys
Available to Purchase
Alloy Digest (2005) 54 (4): Cu-733.
Published: 01 April 2005
Abstract
View articletitled, MOLDSTAR 18, 21, 22: Aluminum Bronze Alloys
View
PDF
for article titled, MOLDSTAR 18, 21, 22: Aluminum Bronze Alloys
MoldStar 18 has good bearing qualities and has resistance to wear, abrasion, fatigue, deformation, and corrosion. MoldStar 21 and 22 are harder alloys and also have good bearing qualities and resistance to wear, abrasion, fatigue, deformation, and corrosion. This family of aluminum bronzes is used as wear plates, sleeve bearings, and guide pin bushings. MoldStar 18 is also known as PAS 18. This datasheet provides information on physical properties, hardness, elasticity, tensile properties, and compressive strength. Filing Code: CU-733. Producer or source: Performance Alloys.
Journal Articles
BRUSHBRONZE 95510: Aluminum Nickel Bronze
Available to Purchase
Alloy Digest (2004) 53 (8): Cu-722.
Published: 01 August 2004
Abstract
View articletitled, BRUSHBRONZE 95510: Aluminum Nickel Bronze
View
PDF
for article titled, BRUSHBRONZE 95510: Aluminum Nickel Bronze
BrushBronze 95510 is an aluminum nickel bronze alloy that combines high strength, ductility, and good abrasion resistance under severe loading conditions. This material, specified as AMS 4880, is frequently used for very demanding aerospace applications. This datasheet provides information on composition, microstructure, and tensile properties. Filing Code: CU-722. Producer or source: Brush Wellman Inc.
Journal Articles
OLIN C638: Bronze Alloy
Available to Purchase
Alloy Digest (2000) 49 (3): Cu-648.
Published: 01 March 2000
Abstract
View articletitled, OLIN C638: Bronze Alloy
View
PDF
for article titled, OLIN C638: Bronze Alloy
Olin C638 is a bronze with additions of aluminum, silicon, and cobalt to give a combination of strength, weldability, contact resistance, and corrosion resistance. It is typically used in springs, switch parts, and contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-648. Producer or source: Olin Brass.
Journal Articles
AMPCO-TRODE 300: Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
Abstract
View articletitled, AMPCO-TRODE 300: Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 300: Aluminum Bronze Filler Metal
AMPCO-TRADE 300 has a very high hardness and yield strength and is used for new or rebuilding of ferrous dies. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-596. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 46: Nickel Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1994) 43 (1): Cu-595.
Published: 01 January 1994
Abstract
View articletitled, AMPCO-TRODE 46: Nickel Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 46: Nickel Aluminum Bronze Filler Metal
AMPCO-TRODE 46 is recommended for cast and wrought nickel-aluminum bronze. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-595. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 40: Manganese-Nickel-Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1993) 42 (12): Cu-593.
Published: 01 December 1993
Abstract
View articletitled, AMPCO-TRODE 40: Manganese-Nickel-Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 40: Manganese-Nickel-Aluminum Bronze Filler Metal
AMPCO-TRODE 40 is a manganese-nickel-aluminum bronze for welding ship propellers and some dissimilar combinations. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-593. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 250: Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1993) 42 (11): Cu-591.
Published: 01 November 1993
Abstract
View articletitled, AMPCO-TRODE 250: Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 250: Aluminum Bronze Filler Metal
AMPCO-TRODE 250 is used in extreme bearing applications and to weld AMPCO 21 castings (See Alloy Digest Cu-93, October 1960). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-591. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 200: Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1993) 42 (8): Cu-586.
Published: 01 August 1993
Abstract
View articletitled, AMPCO-TRODE 200: Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 200: Aluminum Bronze Filler Metal
AMPCO-TRODE 200 is both filler metal and electrodes for extreme wear and high pressures in bearing overlays. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-586. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 150: Aluminum Bronze Filler Metal
Available to Purchase
Alloy Digest (1993) 42 (7): Cu-585.
Published: 01 July 1993
Abstract
View articletitled, AMPCO-TRODE 150: Aluminum Bronze Filler Metal
View
PDF
for article titled, AMPCO-TRODE 150: Aluminum Bronze Filler Metal
AMPCO-TRODE 150 is recommended for overlay application and welding AMPCO 18 alloy (Alloy Digest Cu-51, June 1957). This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-585. Producer or source: Ampco Metal Inc.
Journal Articles
AMPCO-TRODE 160: Aluminum Bronze Coated Electrodes
Available to Purchase
Alloy Digest (1993) 42 (6): Cu-584.
Published: 01 June 1993
Abstract
View articletitled, AMPCO-TRODE 160: Aluminum Bronze Coated Electrodes
View
PDF
for article titled, AMPCO-TRODE 160: Aluminum Bronze Coated Electrodes
AMPCO-TRODE 160 is an aluminum bronze coated electrode that produces deposits with a good combination of strength, ductility and hardness. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: CU-584. Producer or source: Ampco Metal Inc.