Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-17 of 17
Red brass
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2021) 70 (10): Cu-925.
Published: 01 October 2021
Abstract
View articletitled, WIELAND C23000: 85Cu-15Zn Alloy
View
PDF
for article titled, WIELAND C23000: 85Cu-15Zn Alloy
Wieland C23000 (C230), also known as red brass, is an 85Cu-15Zn alloy. The alloy has excellent cold forming properties and is generally not susceptible to dezincification and stress corrosion. Due to this combination of properties and its attractive color, the alloy is used for decorative purposes as well as for a wide variety of drawn and formed parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating. Filing Code: Cu-925. Producer or source: Wieland Rolled Products NA.
Journal Articles
Alloy Digest (2018) 67 (2): Cu-868.
Published: 01 February 2018
Abstract
View articletitled, WIELAND-G05: Leaded Red Brass
View
PDF
for article titled, WIELAND-G05: Leaded Red Brass
Wieland-G05 is cast leaded red brass with excellent corrosion resistance and machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, and joining. Filing Code: Cu-868. Producer or source: Wieland Metals Inc..
Journal Articles
Alloy Digest (2002) 51 (12): Cu-694.
Published: 01 December 2002
Abstract
View articletitled, WIELAND-M15: Brass Alloy
View
PDF
for article titled, WIELAND-M15: Brass Alloy
Wieland-M15 is copper-zinc alloy with good electrical conductivity and a red color useful in decorative applications. The alloy has also been called red brass, 85%, and CA 230. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-694. Producer or source: Wieland Metals Inc., Wieland-Werke AG.
Journal Articles
Alloy Digest (1996) 45 (7): Cu-606.
Published: 01 July 1996
Abstract
View articletitled, SEBILOY II: Low-Lead Red Brass Casting Alloy
View
PDF
for article titled, SEBILOY II: Low-Lead Red Brass Casting Alloy
SeBiLOY II (UNS C89520) is a selenium/bismuth-modified cast red brass alloy. Its low lead content helps meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The Se/Bi modification permits machining exactly like the leaded red brasses it is replacing. This datasheet provides information on composition and physical properties. It also includes information on casting, machining, and joining. Filing Code: CU-606. Producer or source: Copper alloy producers.
Journal Articles
Alloy Digest (1996) 45 (6): Cu-605.
Published: 01 June 1996
Abstract
View articletitled, SEBILOY I: Low-Lead Red Brass Casting Alloy
View
PDF
for article titled, SEBILOY I: Low-Lead Red Brass Casting Alloy
SeBiLOY I (UNS C89510) is a selenium/bismuth-modified cast red brass alloy. Its low lead content helps meet the National Sanitation Foundation’s standard on low lead pickup in water supply systems. The Se/Bi modification permits machining similar to some of the red brasses it is replacing. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, machining, and joining. Filing Code: CU-605. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1990) 39 (12): Cu-556.
Published: 01 December 1990
Abstract
View articletitled, COPPER ALLOY No. C32000: Leaded Red Brass
View
PDF
for article titled, COPPER ALLOY No. C32000: Leaded Red Brass
Copper alloy C32000 is a leaded red brass applicable to automatic screw machine production of parts for hardware and industrial applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-556. Producer or source: Copper and copper alloy mills.
Journal Articles
Alloy Digest (1988) 37 (12): Cu-543.
Published: 01 December 1988
Abstract
View articletitled, UNS C83600: Cast Leaded Red Brass
View
PDF
for article titled, UNS C83600: Cast Leaded Red Brass
UNS C83600 is a free-cutting copper-tin-lead-zinc casting alloy. It offers good casting characteristics but soundness is poor in large castings. It has moderate strength and ductility, and good resistance to corrosion. It is used widely for such applications as valves, gears and general hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-543. Producer or source: Copper alloy producers.
Journal Articles
Alloy Digest (1983) 32 (4): Cu-457.
Published: 01 April 1983
Abstract
View articletitled, COPPER ALLOY No. C84800: Cast Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. C84800: Cast Semi Red Brass
Copper Alloy C84800 is a copper-tin-lead-zinc alloy. It was identified formerly as 76-21/2-61/2-15 alloy for Leaded Semi-Red Brass. It has good casting properties, free-cutting characteristics, moderate strength and ductility and good resistance to corrosion. Its applications include plumbing fixtures, faucets and general hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-457. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1983) 32 (3): Cu-455.
Published: 01 March 1983
Abstract
View articletitled, ANACONDA ALLOY 230: Red Brass
View
PDF
for article titled, ANACONDA ALLOY 230: Red Brass
ANACONDA Alloy 230 is a single-phase brass containing nominally 85% copper and 15% zinc. It is the most widely used of the low-zinc brasses. It has excellent resistance to dezincification and season cracking. Generally it is considered to be the most durable of all alloys for commercial water pipe in the practical price range. Other uses include architectural components, electrical conduit, paper rolls, razor handles and costume jewelry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-455. Producer or source: Anaconda American Brass Company.
Journal Articles
Alloy Digest (1982) 31 (12): Cu-450.
Published: 01 December 1982
Abstract
View articletitled, COPPER ALLOY No. C84200: Cast Leaded Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. C84200: Cast Leaded Semi Red Brass
Copper Alloy No.1 C84200 is a free-machining copper-tin-lead-zinc alloy for castings; it was formerly identified as 80-5-2.5-12.5 alloy. It has good casting characteristics, good machinability, moderate strength and ductility and good corrosion resistance. Among its many uses are ornamental fixtures, general hardware, plumbing goods, small gears and pipe fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-450. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-446, October 1982.
Journal Articles
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
Abstract
View articletitled, COPPER ALLOY No. C84200: Cast Leaded Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. C84200: Cast Leaded Semi Red Brass
Copper Alloy No. C84200 is a free-cutting copper-zinc-tin-lead alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. Formerly used named (not recommended) are 101, Leaded Semi-Red Brass and 80-5-2.5-12.5. Typical applications are pipe fittings, bushings, locknuts and unions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-446. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-450, December 1982.
Journal Articles
Alloy Digest (1979) 28 (8): Cu-378.
Published: 01 August 1979
Abstract
View articletitled, COPPER ALLOY No. 845: Cast Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. 845: Cast Semi Red Brass
Copper Alloy No. 845 was formerly identified as 78-3-7-12 alloy or 78 Semi-Red Brass. It is a free-cutting copper-tin-lead-zinc alloy and is characterized by good casting properties, moderate strength and ductility, excellent machinability and good corrosion resistance. Among its many uses are low-pressure valve fittings, plumbing fixtures and general hardware fittings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-378. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1978) 27 (3): Cu-349.
Published: 01 March 1978
Abstract
View articletitled, COPPER ALLOY No. 844: Cast Leaded Semi Red Brass
View
PDF
for article titled, COPPER ALLOY No. 844: Cast Leaded Semi Red Brass
Copper Alloy No. 844 is a free-cutting copper-tin-lead-zinc alloy for castings; it was formerly identified as 81-3-7-9 alloy. It is characterized by good casting properties, moderate strength and ductility, good machinability and good resistance to corrosion. It is used widely for fittings, plumbing goods and valves. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-349. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1978) 27 (1): Cu-346.
Published: 01 January 1978
Abstract
View articletitled, COPPER ALLOY No. 838: Cast Leaded Red Brass
View
PDF
for article titled, COPPER ALLOY No. 838: Cast Leaded Red Brass
Copper Alloy No. 838 is a free-cutting copper-base alloy for castings. It was formerly identified as Commercial Red Brass or 83-4-6-7 alloy. It offers an excellent combination of corrosion resistance, machinability, moderate strength and good casting characteristics. Its wide use includes such applications as plumbing goods, ornaments and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-346. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1976) 25 (8): Cu-317.
Published: 01 August 1976
Abstract
View articletitled, COPPER ALLOY No. 836: Cast Leaded Red Brass
View
PDF
for article titled, COPPER ALLOY No. 836: Cast Leaded Red Brass
Copper Alloy No. 836 is a free-cutting copper-tin-lead-zinc alloy for castings. It offers good casting characteristics, moderate strength and ductility, good machinability and good resistance to corrosion. It is used widely for such applications as valves, gears and general hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-317. Producer or source: Copper alloy foundries.
Journal Articles
Alloy Digest (1972) 21 (3): Cu-252.
Published: 01 March 1972
Abstract
View articletitled, COPPER ALLOY No. 230: Copper Zinc Alloy
View
PDF
for article titled, COPPER ALLOY No. 230: Copper Zinc Alloy
COPPER ALLOY No. 230 is a single-phase brass containing 15% zinc which is the most widely used of the low zinc brasses. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-252. Producer or source: Brass mills.
Journal Articles
Alloy Digest (1961) 10 (7): Cu-103.
Published: 01 July 1961
Abstract
View articletitled, RED BRASS 85%: Corrosion Resistant Brass
View
PDF
for article titled, RED BRASS 85%: Corrosion Resistant Brass
RED BRASS, 85% is a copper-zinc alloy having high corrosion resistance to water and high resistance to stress-cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-103. Producer or source: Brass mills.