Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 79
Wrought aluminum alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
AUSTRAL WRIGHT 5251: Al-2.0Mg-0.3Mn Alloy
Available to Purchase
Alloy Digest (2023) 72 (2): Al-494.
Published: 01 February 2023
Abstract
View articletitled, AUSTRAL WRIGHT 5251: Al-2.0Mg-0.3Mn Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 5251: Al-2.0Mg-0.3Mn Alloy
Austral Wright 5251 is a wrought, non-heat-treatable, aluminum-magnesium-manganese alloy (5xxx series). It is about mid-way in the series of aluminum-magnesium alloys for alloying content and strength, which is very similar to that of alloy 5052. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-494. Producer or source: Austral Wright Metals.
Journal Articles
AUSTRAL WRIGHT 5083: Al-4.5Mg-0.7Mn-0.15Cr Alloy
Available to Purchase
Alloy Digest (2023) 72 (1): Al-493.
Published: 01 January 2023
Abstract
View articletitled, AUSTRAL WRIGHT 5083: Al-4.5Mg-0.7Mn-0.15Cr Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 5083: Al-4.5Mg-0.7Mn-0.15Cr Alloy
Austral Wright 5083 is a wrought, non-heat-treatable, aluminum-magnesium-manganese-chromium alloy (5xxx series). It has the highest strength of the non-heat-treatable alloys but is not recommended for use at temperatures in excess of 65 °C (150 °F). It is among the most widely used aluminum alloys for marine applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Al-493. Producer or source: Austral Wright Metals.
Journal Articles
AUSTRAL WRIGHT 5052: Al-2.5Mg-0.25Cr Alloy
Available to Purchase
Alloy Digest (2022) 71 (12): Al-492.
Published: 01 December 2022
Abstract
View articletitled, AUSTRAL WRIGHT 5052: Al-2.5Mg-0.25Cr Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 5052: Al-2.5Mg-0.25Cr Alloy
Austral Wright 5052 is a wrought, non-heat-treatable, aluminum-magnesium-chromium alloy (5xxx series) that exhibits a good combination of strength, corrosion resistance, and formability in a wide range of rolled products. It is about mid-way through the series of aluminum-magnesium alloys for alloying content and strength. It has excellent fatigue properties, with an endurance limit of 115 MPa in the H32 temper and 125 MPa in the H34 temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-492. Producer or source: Austral Wright Metals.
Journal Articles
AUSTRAL WRIGHT 5005: Al-0.8Mg Alloy
Available to Purchase
Alloy Digest (2022) 71 (8): Al-489.
Published: 01 August 2022
Abstract
View articletitled, AUSTRAL WRIGHT 5005: Al-0.8Mg Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 5005: Al-0.8Mg Alloy
Austral Wright 5005 is a wrought, non-heat-treatable, aluminum-magnesium alloy (5xxx series) that exhibits moderate strength, good formability, and good resistance to corrosion in marine atmospheres. It is widely used for decorative and architectural applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-489. Producer or source: Austral Wright Metals.
Journal Articles
ATLAS 6063: Al-0.7Mg-0.4Si Alloy
Available to Purchase
Alloy Digest (2022) 71 (7): Al-488.
Published: 01 July 2022
Abstract
View articletitled, ATLAS 6063: Al-0.7Mg-0.4Si Alloy
View
PDF
for article titled, ATLAS 6063: Al-0.7Mg-0.4Si Alloy
Atlas 6063 is a wrought, heat-treatable, aluminum-magnesium-silicon extrusion alloy (6xxx series) that offers good mechanical properties. It responds well to polishing, chemical brightening, anodizing, and dyeing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-488. Producer or source: Atlas Steels.
Journal Articles
AUSTRAL WRIGHT 3003: Al-1.25Mn-0.12Cu Alloy
Available to Purchase
Alloy Digest (2022) 71 (2): Al-485.
Published: 01 February 2022
Abstract
View articletitled, AUSTRAL WRIGHT 3003: Al-1.25Mn-0.12Cu Alloy
View
PDF
for article titled, AUSTRAL WRIGHT 3003: Al-1.25Mn-0.12Cu Alloy
Austral Wright 3003 (UNS A93003) is a wrought, non-heat-treatable, aluminum-manganese-copper alloy (3xxx series). It is used in a wide variety of applications where moderate strength, good formability, and good resistance to corrosion are important. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joinability. Filing Code: Al-485. Producer or source: Austral Wright Metals.
Journal Articles
ATLAS 5251: Al–2Mg–0.3Mn Alloy
Available to Purchase
Alloy Digest (2022) 71 (1): Al-484.
Published: 01 January 2022
Abstract
View articletitled, ATLAS 5251: Al–2Mg–0.3Mn Alloy
View
PDF
for article titled, ATLAS 5251: Al–2Mg–0.3Mn Alloy
Atlas 5251 is a wrought, non-heat-treatable, aluminum-magnesium alloy (5xxx series). Alloy 5251, registered in 1972, is essentially the same as the old N4 alloy and is produced primarily in Europe for a variety of common alloy applications. It offers properties similar to those of alloy 5052 for the same temper. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-484. Producer or source: Atlas Steels.
Journal Articles
ATLAS 5052: Wrought Al-2.5Mg-0.25Cr Alloy
Available to Purchase
Alloy Digest (2020) 69 (11): Al-470.
Published: 01 November 2020
Abstract
View articletitled, ATLAS 5052: Wrought Al-2.5Mg-0.25Cr Alloy
View
PDF
for article titled, ATLAS 5052: Wrought Al-2.5Mg-0.25Cr Alloy
Atlas 5052 is a wrought, non-heat-treatable, Al-2.5Mg-0.25Cr alloy (5xxx series) that offers an attractive combination of moderate strength, good formability and weldability, and excellent corrosion resistance particularly in marine atmospheres. It is also very easy to anodize, providing a pleasant matte finish. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-470. Producer or source: Atlas Steels.
Journal Articles
KAISER ALLOY 1100: Commercially Pure Aluminum
Available to Purchase
Alloy Digest (2019) 68 (11): Al-459.
Published: 01 November 2019
Abstract
View articletitled, KAISER ALLOY 1100: Commercially Pure Aluminum
View
PDF
for article titled, KAISER ALLOY 1100: Commercially Pure Aluminum
Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: Al-459. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
PERALUMAN 300: High-Strength Alloy
Available to Purchase
Alloy Digest (2017) 66 (3): Al-454.
Published: 01 March 2017
Abstract
View articletitled, PERALUMAN 300: High-Strength Alloy
View
PDF
for article titled, PERALUMAN 300: High-Strength Alloy
PERALUMAN 300 is a 5754 aluminum alloy in the wrought aluminum-magnesium family (5000 or 5xxx series). It is closely related to the alloys 5154 and 5454 (Aluminum Association designations that only differ in the second digit are variations on the same alloy). Of the three 5x54 alloys, 5754 is the least alloyed (highest composition % of aluminum), but only by a small amount. It is used in similar applications. As wrought alloy, it can be formed by rolling, extrusion, and forging, but not casting. It can be cold worked to produce tempers with a higher strength but a lower ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance and surface qualities as well as forming, machining, and joining. Filing Code: Al-454. Producer or source: Lamineries Matthey SA.
Journal Articles
KAISER ALLOY 7033: High Strength Forgings
Available to Purchase
Alloy Digest (2011) 60 (6): Al-437.
Published: 01 June 2011
Abstract
View articletitled, KAISER ALLOY 7033: High Strength Forgings
View
PDF
for article titled, KAISER ALLOY 7033: High Strength Forgings
Kaiser Alloy 7033 is a high strength alloy used in automotive frames. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on forming, machining, and joining. Filing Code: Al-437. Producer or source: Kaiser Aluminum.
Journal Articles
KUBOTA ALLOY CH-20: Corrosion Resistant Stainless Casting
Available to Purchase
Alloy Digest (2011) 60 (3): SS-1085.
Published: 01 March 2011
Abstract
View articletitled, KUBOTA ALLOY CH-20: Corrosion Resistant Stainless Casting
View
PDF
for article titled, KUBOTA ALLOY CH-20: Corrosion Resistant Stainless Casting
Kubota Alloy CH-20 (ASTM A743) is an iron-chromium-nickel alloy that has other variations with lower carbon and addition of molybdenum. The nearest wrought equivalent is type 309 stainless. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on casting and joining. Filing Code: SS-1085. Producer or source: Kubota Metal Corporation, Fahramet Division.
Journal Articles
KAISER ALLOY 6063: High Strength Extruded and Drawn Products
Available to Purchase
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
Abstract
View articletitled, KAISER ALLOY 6063: High Strength Extruded and Drawn Products
View
PDF
for article titled, KAISER ALLOY 6063: High Strength Extruded and Drawn Products
Kaiser Alloy 6063 is a magnesium/silicon alloy. One of the most popular of the heat treatable alloy group. Products include extruded and drawn tube, pipe, rod, bar, and profiles. This alloy has good corrosion resistance, good weldability, and a good anodizing response. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-436. Producer or source: Kaiser Aluminum. See also Alloy Digest Al-458, July 2019.
Journal Articles
KAISER ALLOY 7003: Extruded Rod and Bar
Available to Purchase
Alloy Digest (2010) 59 (12): Al-434.
Published: 01 December 2010
Abstract
View articletitled, KAISER ALLOY 7003: Extruded Rod and Bar
View
PDF
for article titled, KAISER ALLOY 7003: Extruded Rod and Bar
Kaiser Alloy 7003 is a medium strength alloy originally developed in Japan. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: AL-434. Producer or source: Kaiser Aluminum.
Journal Articles
ALCOA 7055-T7751 PLATE and T77511 EXTRUSIONS: Aerospace 7xxx Series Aluminum Alloy
Available to Purchase
Alloy Digest (2010) 59 (2): Al-428.
Published: 01 February 2010
Abstract
View articletitled, ALCOA 7055-T7751 PLATE and T77511 EXTRUSIONS: Aerospace 7xxx Series Aluminum Alloy
View
PDF
for article titled, ALCOA 7055-T7751 PLATE and T77511 EXTRUSIONS: Aerospace 7xxx Series Aluminum Alloy
The 7xxx series alloys contain zinc as the main alloying element, usually in combination with magnesium and copper. Alcoa’s high-strength 7055 alloy is supplied as plate and extrusions and used for compressive strength applications. This datasheet provides information on composition, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: AL-428. Producer or source: Alcoa Mill Products Inc.
Journal Articles
ALCAN 6056 T4511/T6511/T78511: Al-Si-Mg-Zn-Cu-Mn Alloy
Available to Purchase
Alloy Digest (2008) 57 (12): Al-419.
Published: 01 December 2008
Abstract
View articletitled, ALCAN 6056 T4511/T6511/T78511: Al-Si-Mg-Zn-Cu-Mn Alloy
View
PDF
for article titled, ALCAN 6056 T4511/T6511/T78511: Al-Si-Mg-Zn-Cu-Mn Alloy
Alcan 6056 alloy is an Al-Si-Mg-Zn-Cu-Mn weldable alloy, developed to provide medium strength similar to the incumbent 2024 alloy, with a lower density. This datasheet covers ALCAN 6056 in several tempers as thin extrusions. The alloy possesses, in several tempers, a superior combination of weldability, high-strength, and corrosion resistance. This datasheet provides information on composition and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: AL-419. Producer or source: Alcan Inc.
Journal Articles
ALCOA 2026: Aluminum Extrusion Alloy
Available to Purchase
Alloy Digest (2006) 55 (10): Al-401.
Published: 01 October 2006
Abstract
View articletitled, ALCOA 2026: Aluminum Extrusion Alloy
View
PDF
for article titled, ALCOA 2026: Aluminum Extrusion Alloy
Alcoa extrusion alloy 2026 was developed as an improvement over 2024 and 2224 extrusions in aerospace structural applications where the governing selection criteria are high damage tolerance, good fatigue resistance, and a high degree of manufacturability. In addition to improved damage tolerance, extrusion alloy 2026-T3511 also has a significantly higher A-basis minimum strength than 2024-T3511 and 2224-T3511. This datasheet provides information on composition, tensile properties, and compressive strength as well as fatigue. It also includes information on corrosion resistance as well as forming. Filing Code: AL-401. Producer or source: AEAP-Alcoa Engineered Aerospace Products.
Journal Articles
ALCOA 6061: Extruded Precipitation-Hardenable Aluminum Alloy
Available to Purchase
Alloy Digest (2006) 55 (1): Al-281.
Published: 01 January 2006
Abstract
View articletitled, ALCOA 6061: Extruded Precipitation-Hardenable Aluminum Alloy
View
PDF
for article titled, ALCOA 6061: Extruded Precipitation-Hardenable Aluminum Alloy
Alloy 6061 is one of the most widely used alloys in the 6000 Series. This data sheet revision adds standard tempers and many of the Alcoa special tempers, as well as properties for extrusions and shapes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: AL-281. Producer or source: Alcoa Engineered Products. Originally published May 1987, revised January 2006.
Journal Articles
GIANTAL: Aluminum Mold Alloy
Available to Purchase
Alloy Digest (2004) 53 (6): Al-390.
Published: 01 June 2004
Abstract
View articletitled, GIANTAL: Aluminum Mold Alloy
View
PDF
for article titled, GIANTAL: Aluminum Mold Alloy
Giantal is a wrought aluminum alloy for mold applications such as low-pressure plastic and composite molding, including thermoforming and resin transfer molding that require the material to have excellent corrosion resistance and weldability. The 5xxx aluminum alloys are preferred for this type of application. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance. Filing Code: AL-390. Producer or source: Corus Aluminum Rolled Products USA.
Journal Articles
ALCOA 7150: High-Strength Aluminum Plate Alloy
Available to Purchase
Alloy Digest (2004) 53 (5): Al-388.
Published: 01 May 2004
Abstract
View articletitled, ALCOA 7150: High-Strength Aluminum Plate Alloy
View
PDF
for article titled, ALCOA 7150: High-Strength Aluminum Plate Alloy
Alcoa alloy 7150 in the T6151 temper is the highest-strength aluminum plate alloy available. The T77 temper provides a combination of very high strength and corrosion resistance. The alloy is a second-generation version of alloy 7050. This datasheet provides information on composition, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating. Filing Code: AL-388. Producer or source: Alcoa Mill Products Inc.