Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Nickel powder
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2011) 60 (4): Ni-689.
Published: 01 April 2011
Abstract
View article
PDF
DELORO 15, 21, 22, and 25 are prealloyed, gas-atomized, nickel-base powders for repair of glass-forming molds. This datasheet provides information on composition, physical properties, and hardness. It also includes information on powder metal forms. Filing Code: Ni-689. Producer or source: Stellite Coatings.
Journal Articles
Alloy Digest (1976) 25 (4): Ni-225.
Published: 01 April 1976
Abstract
View article
PDF
METCO 447 is a nickel-aluminum-molybdenum powder developed to produce self-bonding, low-shrink, moderately hard coatings. It is recommended for resistance to wear and particle erosion, and for the buildup and salvage of both machinable and grindable carbon steels. It is applied in a one-step, single-coat buildup generally by ThermoSpray, but it may be applied by plasma spraying. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as machining, surface treatment, and powder metal forms. Filing Code: Ni-225. Producer or source: Metco Inc..