Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-7 of 7
Spring steel
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (5): SA-496.
Published: 01 May 1998
Abstract
View article
PDF
Inland DuraSpring is a high-strength microalloyed spring steel for use in high stress coil springs for automobile and light truck suspension systems. This bar product offers significant improvements in tensile strength, fatigue properties, and fracture toughness compared to conventional spring steels. This datasheet provides information on composition, hardness, and tensile properties as well asfracture toughness and fatigue. Filing Code: SA-496. Producer or source: Ispat Inland Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (3): SA-223.
Published: 01 March 1968
Abstract
View article
PDF
AISI 9262 is an alloy spring steel of the oil hardening type. It is also used for tough and shock resistant tool application. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-223. Producer or source: Alloy steel mills and foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (3): SA-207.
Published: 01 March 1967
Abstract
View article
PDF
AISI 5160 is a medium-carbon through-hardening alloy steel recommended for heavy duty service in gearing, shafting, tools, hot work dies and springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-207. Producer or source: Alloy steel mills and foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (9): SA-167.
Published: 01 September 1964
Abstract
View article
PDF
AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-167. Producer or source: Alloy steel mills and foundries.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (12): CS-17.
Published: 01 December 1961
Abstract
View article
PDF
AISI C1080 is a high carbon, water or oil hardening tool and spring steel having medium hardness penetration. It is recommended for general purpose tools, springs, and machinery parts requiring high hardness and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-17. Producer or source: Carbon and alloy steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (12): CS-11.
Published: 01 December 1959
Abstract
View article
PDF
AISI C1095 is a high-carbon, water-hardening tool and spring steel having medium hardness penetration. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-11. Producer or source: Carbon and alloy steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (8): SA-73.
Published: 01 August 1958
Abstract
View article
PDF
AISI 9255 is a silico-manganese spring and tool steel having good toughness and shock resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-73. Producer or source: Alloy steel mills and foundries.