Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Tin-based bearing alloys
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
FEDERATED No. 3: Tin-Base Bearing Alloy
Available to Purchase
Alloy Digest (1956) 5 (7): Sn-2.
Published: 01 July 1956
Abstract
View articletitled, FEDERATED No. 3: Tin-Base Bearing Alloy
View
PDF
for article titled, FEDERATED No. 3: Tin-Base Bearing Alloy
FEDRATED NO. 3 is a tin-base bearing alloy recommended for moderate to high speeds and loads. It has low frictional resistance, low wear, good running-in properties, good emergency behavior upon failing of lubrication, and lower coefficient of expension than the lead-base alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Sn-2. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
FEDERATED No. 2: Bearing Alloy
Available to Purchase
Alloy Digest (1954) 3 (10): Sn-1.
Published: 01 October 1954
Abstract
View articletitled, FEDERATED No. 2: Bearing Alloy
View
PDF
for article titled, FEDERATED No. 2: Bearing Alloy
Federated No. 2 is a tin-base white Babbitt metal used for bearings where speeds, loads and stresses are moderate to high. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on casting and joining. Filing Code: Sn-1. Producer or source: Federated Metals Corporation, ASARCO Inc..