Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 190
Dies
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
CRYODUR 2833: Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (10): TS-777.
Published: 01 October 2019
Abstract
View articletitled, CRYODUR 2833: Cold-Work Tool Steel
View
PDF
for article titled, CRYODUR 2833: Cold-Work Tool Steel
Cryodur 2833 is a wear-resistant water-hardening steel with resistance to overheating. Applications include cold heading dies; first and finish upsetting punches; cold stamps; dies for the manufacturing of screws, rivets, and bolts; and compression pistons. This datasheet provides information on composition and physical properties. It also includes information on heat treating. Filing Code: TS-777. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
YSS HAP10: Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (8): TS-773.
Published: 01 August 2019
Abstract
View articletitled, YSS HAP10: Cold-Work Tool Steel
View
PDF
for article titled, YSS HAP10: Cold-Work Tool Steel
YSS HAP10 is a powder metallurgy high-speed tool steel with very high toughness for cold forging dies and fine blanking dies. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-773. Producer or source: Hitachi Metals America Ltd.
Journal Articles
YSS DM: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2018) 67 (9): TS-753.
Published: 01 September 2018
Abstract
View articletitled, YSS DM: Hot Work Tool Steel
View
PDF
for article titled, YSS DM: Hot Work Tool Steel
YSS DM is a hot work stool steel with excellent toughness. Applications include hammer forging dies, aluminum forge dies, forging bolsters, and extrusion die backers. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming. Filing Code: TS-753. Producer or source: Hitachi Metals America Ltd.
Journal Articles
YSS MDC-K: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2018) 67 (5): TS-749.
Published: 01 May 2018
Abstract
View articletitled, YSS MDC-K: Hot Work Tool Steel
View
PDF
for article titled, YSS MDC-K: Hot Work Tool Steel
YSS MDC-K is a hot work tool steel grade for hot forging dies. It is a modification of JIS-SKD8 steel. This datasheet provides information on composition and hardness. It also includes information on heat treating. Filing Code: TS-749. Producer or source: Hitachi Metals America Ltd.
Journal Articles
YSS DAC 55: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2018) 67 (2): TS-747.
Published: 01 February 2018
Abstract
View articletitled, YSS DAC 55: Hot Work Tool Steel
View
PDF
for article titled, YSS DAC 55: Hot Work Tool Steel
YSS DAC 55 is a standard grade for die casting dies. Tool steel for large or squeeze die casting molds with excellent heat crack resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating. Filing Code: TS-747. Producer or source: Hitachi Metals America Ltd.
Journal Articles
YSS DAC 10: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2017) 66 (12): TS-745.
Published: 01 December 2017
Abstract
View articletitled, YSS DAC 10: Hot Work Tool Steel
View
PDF
for article titled, YSS DAC 10: Hot Work Tool Steel
YSS DAC 10 is a high-strength steel for precision die casting and hot-working press dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-745. Producer or source: Hitachi Metals America Ltd.
Journal Articles
MTD 1: Prehardened Engineering Steel
Available to Purchase
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
Abstract
View articletitled, MTD 1: Prehardened Engineering Steel
View
PDF
for article titled, MTD 1: Prehardened Engineering Steel
MTD 1 is a 4140 plate steel modified with slightly higher carbon and a vanadium addition. Vanadium improves graining refinement and, coupled with the higher carbon, promotes hardness and wear resistance. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides information on composition. It also includes information on forming, machining, and joining. Filing Code: SA-793. Producer or source: ArcelorMittal USA, Plate.
Journal Articles
BÖHLER W360 ISOBLOC: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2014) 63 (12): TS-727.
Published: 01 December 2014
Abstract
View articletitled, BÖHLER W360 ISOBLOC: Hot Work Tool Steel
View
PDF
for article titled, BÖHLER W360 ISOBLOC: Hot Work Tool Steel
Böhler (or Boehler) W360 Isobloc is a hot work tool steel developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-727. Producer or source: Böhler Edelstahl GmbH & Company KG.
Journal Articles
MX01: Steel for Forging Dies
Available to Purchase
Alloy Digest (2014) 63 (9): SA-708.
Published: 01 September 2014
Abstract
View articletitled, MX01: Steel for Forging Dies
View
PDF
for article titled, MX01: Steel for Forging Dies
MX01 is a steel grade developed to achieve useful properties to minimize the cost of forging dies. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: SA-708. Producer or source: Industeel USA, LLC.
Journal Articles
SANDMEYER SSC INVAR 36: Low Expansion Iron-Nickel Alloy
Available to Purchase
Alloy Digest (2012) 61 (2): Fe-158.
Published: 01 February 2012
Abstract
View articletitled, SANDMEYER SSC INVAR 36: Low Expansion Iron-Nickel Alloy
View
PDF
for article titled, SANDMEYER SSC INVAR 36: Low Expansion Iron-Nickel Alloy
SSC Invar 36 was developed for use in applications where dimensional stability is essential. It is a nickel-iron alloy with a very low coefficient of thermal expansion from cryogenic temperatures to 200 deg C (390 deg F). It is utilized in aerospace composite tooling and die applications, as well as laser components, and cryogenic components and piping: liquefied natural gas production, storage, and transportation. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Fe-158. Producer or source: Sandmeyer Steel Company. Originally published December 2011, revised February 2012.
Journal Articles
DH31-EX: Hot Work Die Steel
Available to Purchase
Alloy Digest (2011) 60 (1): TS-696.
Published: 01 January 2011
Abstract
View articletitled, DH31-EX: Hot Work Die Steel
View
PDF
for article titled, DH31-EX: Hot Work Die Steel
DH31-EX was developed to extend the life of aluminum die cast dies, and other hot forging or pressing dies. This datasheet provides information on physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-696. Producer or source: International Mold Steel Inc..
Journal Articles
THERMODUR 2714: Hot Work Tool Steel
Available to Purchase
Alloy Digest (2010) 59 (11): TS-694.
Published: 01 November 2010
Abstract
View articletitled, THERMODUR 2714: Hot Work Tool Steel
View
PDF
for article titled, THERMODUR 2714: Hot Work Tool Steel
Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing Code: TS-694. Producer or source: Schmolz + Bickenbach USA Inc.
Journal Articles
KAPSTAR: Die-Casting Tool Steel
Available to Purchase
Alloy Digest (2009) 58 (11): TS-684.
Published: 01 November 2009
Abstract
View articletitled, KAPSTAR: Die-Casting Tool Steel
View
PDF
for article titled, KAPSTAR: Die-Casting Tool Steel
Kapstar is through-hardened steel of uniform hardness for molds and dies. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and joining. Filing Code: TS-684. Producer or source: Crucible Service Centers Divisional Headquarters.
Journal Articles
DURATECH PYROVAN HC: Powder Metal Tool Steel
Available to Purchase
Alloy Digest (2008) 57 (7): TS-667.
Published: 01 July 2008
Abstract
View articletitled, DURATECH PYROVAN HC: Powder Metal Tool Steel
View
PDF
for article titled, DURATECH PYROVAN HC: Powder Metal Tool Steel
DuraTech Pyrovan HC is air hardened and has a combination of strength, wear resistance, and toughness for use in blanking and sizing dies. The alloy is made by powder metallurgy. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on heat treating, machining, and powder metal forms. Filing Code: TS-667. Producer or source: Latrobe Specialty Steel Company.
Journal Articles
TOUGHTEC SF: Cold Work Tool Steel
Available to Purchase
Alloy Digest (2007) 56 (5): TS-648.
Published: 01 May 2007
Abstract
View articletitled, TOUGHTEC SF: Cold Work Tool Steel
View
PDF
for article titled, TOUGHTEC SF: Cold Work Tool Steel
Toughtec SF is a spray-formed cold-work tool steel offering a combination of high wear resistance and very good ductility. Toughtec SF is suitable for the production of hot shearing dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-648. Producer or source: Böhler-Uddeholm North America.
Journal Articles
CARPENTER MICRO-MELT M48: Superhigh-Speed Steel
Available to Purchase
Alloy Digest (2005) 54 (11): TS-622.
Published: 01 November 2005
Abstract
View articletitled, CARPENTER MICRO-MELT M48: Superhigh-Speed Steel
View
PDF
for article titled, CARPENTER MICRO-MELT M48: Superhigh-Speed Steel
Micro-Melt M48 alloy is a superhigh-speed tool steel with a high alloy content and capable of achieving a hardness of 70 HRC. The alloy is used in various tooling and die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-622. Producer or source: Carpenter Specialty Alloys.
Journal Articles
DRM3: Cold Forging Die Steel
Available to Purchase
Alloy Digest (2005) 54 (9): TS-619.
Published: 01 September 2005
Abstract
View articletitled, DRM3: Cold Forging Die Steel
View
PDF
for article titled, DRM3: Cold Forging Die Steel
Daido DRM3 is a high-speed tool steel with both high hardness (66 HRC maximum) and toughness for improved life in dies. The alloy has excellent hardenability. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-619. Producer or source: International Mold Steel Inc., Daido Steel.
Journal Articles
DRM2: High-Speed Tool Steel
Available to Purchase
Alloy Digest (2005) 54 (8): TS-618.
Published: 01 August 2005
Abstract
View articletitled, DRM2: High-Speed Tool Steel
View
PDF
for article titled, DRM2: High-Speed Tool Steel
Daido DRM2 is a high-speed tool steel with both high hardness (62 HRC maximum) and toughness for improved life in dies. The alloy is a matrix type for warm and cold forging tools. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fatigue. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-618. Producer or source: International Mold Steel Inc., Daido Steel.
Journal Articles
CRUCIBLE S7 XL: Shock-Resisting Tool Steel
Available to Purchase
Alloy Digest (2005) 54 (4): TS-562.
Published: 01 April 2005
Abstract
View articletitled, CRUCIBLE S7 XL: Shock-Resisting Tool Steel
View
PDF
for article titled, CRUCIBLE S7 XL: Shock-Resisting Tool Steel
Crucible S7 XL is a double-refined high-purity grade of S7 tool steel (see Alloy Digest TS-543, July 1996) designed specifically for ease of wire electrical discharge machining (EDM) operations, improved consistency in texturizing of plastic injection molds, and superior shock resistance compared to conventional S7. Typical applications include plastic injection molds, punches and dies by wire EDM, and heavy impact tools. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: TS-562. Producer or source: Crucible Service Centers. Originally published November 1998, revised 2005.
Journal Articles
CRU-WEAR: Air Hardening Tool Steel
Available to Purchase
Alloy Digest (2001) 50 (11): TS-592.
Published: 01 November 2001
Abstract
View articletitled, CRU-WEAR: Air Hardening Tool Steel
View
PDF
for article titled, CRU-WEAR: Air Hardening Tool Steel
CRU-WEAR is an air hardening tool steel with wear resistance greater than D2 and toughness approaching A2. Applications include blades, punches and dies. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and joining. Filing Code: TS-592. Producer or source: Crucible.