Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 123
Construction materials
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
STRENX 1100 CR: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (12): SA-859.
Published: 01 December 2019
Abstract
View articletitled, STRENX 1100 CR: Structural Steel
View
PDF
for article titled, STRENX 1100 CR: Structural Steel
Strenx 1100 CR is a cold-rolled structural steel with a minimum yield strength of 1100 MPa (160 ksi) for stronger and lighter structures. This material is available as cut-to-length sheets. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: SA-859. Producer or source: SSAB Swedish Steel, Inc..
Journal Articles
STRENX 1100 PLUS: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (11): SA-856.
Published: 01 November 2019
Abstract
View articletitled, STRENX 1100 PLUS: Structural Steel
View
PDF
for article titled, STRENX 1100 PLUS: Structural Steel
Strenx™ 1100 Plus is a high-strength, hot-rolled, quenched and tempered, structural steel with a minimum yield strength of 1100 MPa (160 ksi) and very good weld performance. The strength, elongation, and impact toughness of weldments fulfill minimum guarantees of the base metal. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-856. Producer or source: SSAB Swedish Steel, Inc..
Journal Articles
BISALLOY STRUCTURAL 80 PRESSURE VESSEL STEEL: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (5): SA-844.
Published: 01 May 2019
Abstract
View articletitled, BISALLOY STRUCTURAL 80 PRESSURE VESSEL STEEL: Structural Steel
View
PDF
for article titled, BISALLOY STRUCTURAL 80 PRESSURE VESSEL STEEL: Structural Steel
Bisalloy Structural 80 Pressure Vessel Steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel for pressure vessel applications. It exhibits excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, machining, and joining. Filing Code: SA-844. Producer or source: Bisalloy Steels Group Limited.
Journal Articles
BISALLOY STRUCTURAL 80: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (4): SA-842.
Published: 01 April 2019
Abstract
View articletitled, BISALLOY STRUCTURAL 80: Structural Steel
View
PDF
for article titled, BISALLOY STRUCTURAL 80: Structural Steel
Bisalloy Structural 80 steel (80 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and joining. Filing Code: SA-842. Producer or source: Bisalloy Steels Group Limited.
Journal Articles
BISALLOY STRUCTURAL 70: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (3): SA-840.
Published: 01 March 2019
Abstract
View articletitled, BISALLOY STRUCTURAL 70: Structural Steel
View
PDF
for article titled, BISALLOY STRUCTURAL 70: Structural Steel
Bisalloy Structural 70 steel (70 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on forming and joining. Filing Code: SA-840. Producer or source: Bisalloy Steels Group Limited.
Journal Articles
STRENX 100: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (2): SA-838.
Published: 01 February 2019
Abstract
View articletitled, STRENX 100: Structural Steel
View
PDF
for article titled, STRENX 100: Structural Steel
Strenx 100 is a high-strength, high-performance structural steel with a minimum yield strength of 690 MPa (100 ksi). It meets the requirements of ASTM A514 Grade S. Strenx 100 is a US Customary steel similar to Strenx 700 (Alloy Digest SA-779, February 2017). This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: SA-838. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
BISALLOY STRUCTURAL 60: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (2): SA-839.
Published: 01 February 2019
Abstract
View articletitled, BISALLOY STRUCTURAL 60: Structural Steel
View
PDF
for article titled, BISALLOY STRUCTURAL 60: Structural Steel
Bisalloy Structural 60 steel (60 ksi minimum yield strength) is a low-carbon, low-alloy, high-strength structural steel exhibiting excellent cold formability and low-temperature fracture toughness. This datasheet provides information on composition and shear strength. It also includes information on forming and joining. Filing Code: SA-839. Producer or source: Bisalloy Steels Group Limited.
Journal Articles
STRENX 1100: Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (1): SA-834.
Published: 01 January 2019
Abstract
View articletitled, STRENX 1100: Structural Steel
View
PDF
for article titled, STRENX 1100: Structural Steel
Strenx 1100 is a structural steel that guarantees a minimum yield strength of 1100 MPa (160 ksi). Strenx 1100 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. Despite its strength, the material is easy to weld and bend. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-834. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
XAR 400W: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2019) 68 (1): SA-836.
Published: 01 January 2019
Abstract
View articletitled, XAR 400W: Wear-Resistant Structural Steel
View
PDF
for article titled, XAR 400W: Wear-Resistant Structural Steel
XAR 400W is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear-resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. It is heat resistant up to 400 deg C. This datasheet provides information on composition and physical properties. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-836. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
XAR 450 Premium: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (12): sa-833.
Published: 01 December 2018
Abstract
View articletitled, XAR 450 Premium: Wear-Resistant Structural Steel
View
PDF
for article titled, XAR 450 Premium: Wear-Resistant Structural Steel
XAR 450 Premium is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-833. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
STRENX 960 PLUS: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (12): sa-832.
Published: 01 December 2018
Abstract
View articletitled, STRENX 960 PLUS: Structural Steel
View
PDF
for article titled, STRENX 960 PLUS: Structural Steel
Strenx 960 PLUS is a high-strength structured strip steel with minimum yield strength of 960 MPa (139 ksi). It provides excellent thickness, accuracy, and surface quality in relation to the strength. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-832. Producer or source: SSAB Inc. and Sweden SSAB AB, SSAB AB.
Journal Articles
XAR 400 Premium: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (11): sa-830.
Published: 01 November 2018
Abstract
View articletitled, XAR 400 Premium: Wear-Resistant Structural Steel
View
PDF
for article titled, XAR 400 Premium: Wear-Resistant Structural Steel
XAR 400 Premium is a special wear-resistant structural steel as thick plate that is water quenched and tempered. These wear-resistant materials last at least five times longer than conventional steels due to their extreme hardness and toughness. This datasheet provides information on composition and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-830. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
STRENX 960: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (11): sa-829.
Published: 01 November 2018
Abstract
View articletitled, STRENX 960: Structural Steel
View
PDF
for article titled, STRENX 960: Structural Steel
Strenx 960 is a structural steel that guarantees a minimum yield strength of up to 960 MPa (139 ksi) depending on thickness. Strenx 960 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures where low weight is needed. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-829. Producer or source: SSAB Inc. .
Journal Articles
STRENX 900 PLUS: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (10): SA-826.
Published: 01 October 2018
Abstract
View articletitled, STRENX 900 PLUS: Structural Steel
View
PDF
for article titled, STRENX 900 PLUS: Structural Steel
Strenx 900 Plus is a structural steel with a minimum yield strength of 900 MPa (131 ksi). Strenx 900 Plus provides a good combination of strength and toughness together with good workshop properties. Typical applications include load-bearing structures, where low weight is needed. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-826. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
STRENX 900: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (9): SA-821.
Published: 01 September 2018
Abstract
View articletitled, STRENX 900: Structural Steel
View
PDF
for article titled, STRENX 900: Structural Steel
Strenx 900 is a structural steel that guarantees a minimum yield strength of up to 900 MPa (131 ksi) depending on thickness. Strenx 900 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. It meets the requirements of EN 10 025-6 for the S890 grade and thicknesses. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-821. Producer or source: SSAB Swedish Steel Inc. and SSAB Tunnplat AB.
Journal Articles
STRENX 700CR: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (8): SA-819.
Published: 01 August 2018
Abstract
View articletitled, STRENX 700CR: Structural Steel
View
PDF
for article titled, STRENX 700CR: Structural Steel
Strenx 700 CR is a cold-rolled structural steel with a minimum yield strength of 700 MPa (102 ksi) used to produce stronger and lighter structures. Strenx 700 CR has good cold forming, welding, and cutting performance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on surface qualities as well as joining. Filing Code: SA-819. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
STRENX 700 MC PLUS: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (7): SA-817.
Published: 01 July 2018
Abstract
View articletitled, STRENX 700 MC PLUS: Structural Steel
View
PDF
for article titled, STRENX 700 MC PLUS: Structural Steel
Strenx 700 MC PLUS is a hot-rolled structural steel made for cold forming, with minimum yield strength of 700 MPa (102 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S700MC in EN 10149-2. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on surface qualities. Filing Code: SA-817. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
STRENX 700 OME: Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (4): SA-815.
Published: 01 April 2018
Abstract
View articletitled, STRENX 700 OME: Structural Steel
View
PDF
for article titled, STRENX 700 OME: Structural Steel
Strenx 700 OME is a structural steel with a minimum yield strength of 700 MPa (102 ksi) developed for use in demanding load-bearing structures within the offshore and marine industry. Strenx 700 OME exceeds the requirements of S690QL, EN 10 025-6. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on machining and joining. Filing Code: SA-815. Producer or source: SSAB Swedish Steel Inc..
Journal Articles
TBL PLUS: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (2): SA-811.
Published: 01 February 2018
Abstract
View articletitled, TBL PLUS: Wear-Resistant Structural Steel
View
PDF
for article titled, TBL PLUS: Wear-Resistant Structural Steel
TBL Plus is a wear-resistant special structural steel with boron as heavy plate that is normalized with thicknesses up to 12 mm (in.) made of fine-grained structural steel. This datasheet provides information on composition and tensile properties. It also includes information on wear resistance as well as forming and heat treating. Filing Code: SA-811. Producer or source: ThyssenKrupp Steel Europe AG.
Journal Articles
TBL: Wear-Resistant Structural Steel
Available to Purchase
Alloy Digest (2018) 67 (1): SA-808.
Published: 01 January 2018
Abstract
View articletitled, TBL: Wear-Resistant Structural Steel
View
PDF
for article titled, TBL: Wear-Resistant Structural Steel
TBL is a wear-resistant special structural steel with boron as heavy plate that is normalized with thicknesses up to 100 mm (3.9 in.) made of fine-grained structural steel TBL. This datasheet provides information on composition and tensile properties. It also includes information on forming and heat treating. Filing Code: SA-808. Producer or source: ThyssenKrupp Steel Europe AG.
1