Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-4 of 4
Glass products and materials
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (4): Cr-3.
Published: 01 April 1993
Abstract
View article
PDF
DUCROPUR P/M CHROMIUM is a heat and corrosion resistant P/M chromium material designed for engineering into parts in the chemical and petro-chemical markets, as combustion systems, for use in the glass industry, and as heat exchangers for sulfur containing flue gases. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as machining. Filing Code: CR-3. Producer or source: Metallwerk Plansee.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (12): Fe-60.
Published: 01 December 1979
Abstract
View article
PDF
TECHALLOY GLASSEAL 29-17 is an iron-nickel-cobalt alloy with a thermal expansion rate that is unlike most metals and closely matches the thermal expansion characteristics of borosilicate glass, PYREX glass, and other similar low-expansion materials. It assures precisely controlled expansion properties that are ideal for usage in glass-to-metal seals. Typical applications are transmitting tubes, relays and electronic power tube envelopes. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Fe-60. Producer or source: Techalloy Company Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (3): Ni-242.
Published: 01 March 1977
Abstract
View article
PDF
COLMONOY No. 22 is a nickel-base alloy supplied as atomized powder, welding rod and investment castings. The powder is applied with Colmonoy's FUSEWELD process to repair cast-iron parts. The investment castings are used in the glass industry as forming tools (plungers, baffles and sleeves) and as welding rod for repairing cast-iron glass-container molds and components. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion and wear resistance as well as heat treating, machining, joining, and powder metal forms. Filing Code: Ni-242. Producer or source: Wall Colmonoy Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1977) 26 (1): Ni-239.
Published: 01 January 1977
Abstract
View article
PDF
COLMONOY No. 23A and No. 24 comprise two grades of one nickel-base alloy. The two grades arise from differences in the physical characteristics of the two alloy powders which are applied with Colmonoy's FUSEWELD process. No. 23A is superior for repairing surface flaws of cast-iron components and No. 24 is superior for building-up edges or corners of cast-iron components, such as used in the glass industry. This datasheet provides information on composition, physical properties, and hardness. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: Ni-239. Producer or source: Wall Colmonoy Corporation.