Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 206
High-speed tool steel
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
UDDEHOLM VANADIS 60 SUPERCLEAN: High-Speed Tool Steel
Available to Purchase
Alloy Digest (2022) 71 (1): TS-823.
Published: 01 January 2022
Abstract
View articletitled, UDDEHOLM VANADIS 60 SUPERCLEAN: High-Speed Tool Steel
View
PDF
for article titled, UDDEHOLM VANADIS 60 SUPERCLEAN: High-Speed Tool Steel
Uddeholm Vanadis 60 SuperClean is a cobalt-bearing high-speed tool steel that is produced by the powder metallurgy process. It is suitable for demanding cold work applications and for cutting tools, where the highest wear resistance and highest compressive strength are required at the same time. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-823. Producer or source: Uddeholms AB.
Journal Articles
UDDEHOLM VANADIS 23 SUPERCLEAN: High Speed Tool Steel
Available to Purchase
Alloy Digest (2021) 70 (11): TS-820.
Published: 01 November 2021
Abstract
View articletitled, UDDEHOLM VANADIS 23 SUPERCLEAN: High Speed Tool Steel
View
PDF
for article titled, UDDEHOLM VANADIS 23 SUPERCLEAN: High Speed Tool Steel
Uddeholm Vanadis 23 SuperClean is a chromium-molybdenum-tungsten-vanadium high speed tool steel that is produced by the powder metallurgy process. This steel is similar to Type M3, Class 2 high speed tool steel, and combines high compressive strength with good abrasive wear resistance. It is suitable for demanding cold work applications like blanking of harder materials like carbon steel or cold rolled strip steel and for cutting tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating, machining, and surface treatment. Filing Code: TS-820. Producer or source: Uddeholms AB (a voestalpine company).
Journal Articles
CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
Available to Purchase
Alloy Digest (2021) 70 (9): TS-818.
Published: 01 September 2021
Abstract
View articletitled, CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
View
PDF
for article titled, CRUCIBLE CPM REX 54 HS: Molybdenum-Type High-Speed Tool Steel
Crucible CPM Rex 54 HS is a cobalt-bearing high speed tool steel that is produced by the proprietary Crucible Particle Metallurgy (CPM) process. It combines the wear properties of the popular high vanadium M4 grade with the red hardness of the cobalt-bearing M35/Crucible CPM Rex 45 HS grades. Crucible CPM Rex 54 HS may be used as an upgrade for improved red hardness over M3 or M4 without giving up the abrasion resistance, or as an upgrade for improved wear resistance over M35 or Crucible CPM Rex 45 HS without giving up the red hardness. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also includes information on wear resistance as well as heat treating and surface treatment. Filing Code: TS-818. Producer or source: Crucible Industries LLC.
Journal Articles
CRUCIBLE REX M4: Molybdenum-Type High-Speed Tool Steel
Available to Purchase
Alloy Digest (2021) 70 (4): TS-812.
Published: 01 April 2021
Abstract
View articletitled, CRUCIBLE REX M4: Molybdenum-Type High-Speed Tool Steel
View
PDF
for article titled, CRUCIBLE REX M4: Molybdenum-Type High-Speed Tool Steel
Crucible REX M4 is a special-purpose high-speed tool steel that is designed to provide high wear resistance in tools. Its high vanadium and carbon content provides superior resistance to cratering and wear in cold work punches, die inserts, and cutting applications involving high speed and light cuts. It is designed to give maximum performance while working with abrasive materials, exhibiting better wear resistance than Types M2 or M3. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-812. Producer or source: Crucible Industries LLC.
Journal Articles
CRUCIBLE REX M2: Molybdenum-Type High-Speed Tool Steel
Available to Purchase
Alloy Digest (2020) 69 (10): TS-801.
Published: 01 October 2020
Abstract
View articletitled, CRUCIBLE REX M2: Molybdenum-Type High-Speed Tool Steel
View
PDF
for article titled, CRUCIBLE REX M2: Molybdenum-Type High-Speed Tool Steel
Crucible Rex M2 is a general-purpose high-speed tool steel that contains tungsten, molybdenum, chromium, and vanadium as principal alloying elements. It is suitable for a wide variety of cutting tools that require moderate feeds and speeds. For cold work applications, Rex M2 offers higher hardness and wear resistance than Type D2 tool steel. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-801. Producer or source: Crucible Industries LLC.
Journal Articles
YSS YXR7: High-Speed Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (12): TS-783.
Published: 01 December 2019
Abstract
View articletitled, YSS YXR7: High-Speed Tool Steel
View
PDF
for article titled, YSS YXR7: High-Speed Tool Steel
YSS YXR7 is a high-speed tool steel with good toughness and wear resistance. It is used for blanking dies, forging dies, heading dies, and thread forming dies. This datasheet provides information on composition, physical properties, hardness, and bend strength. It also includes information on heat treating. Filing Code: TS-783. Producer or source: Hitachi Metals America, Ltd.
Journal Articles
YSS YXM4: High-Speed Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (11): TS-780.
Published: 01 November 2019
Abstract
View articletitled, YSS YXM4: High-Speed Tool Steel
View
PDF
for article titled, YSS YXM4: High-Speed Tool Steel
YSS YXM4 is a cobalt-alloyed molybdenum high-speed tool steel with resistance to abrasion, seizure, and deformation under high pressure. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance. Filing Code: TS-780. Producer or source: Hitachi Metals America, Ltd.
Journal Articles
YSS HAP72: P/M High-Speed Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (10): TS-779.
Published: 01 October 2019
Abstract
View articletitled, YSS HAP72: P/M High-Speed Tool Steel
View
PDF
for article titled, YSS HAP72: P/M High-Speed Tool Steel
YSS HAP72 is a powder metallurgy high-speed tool steel with a very high wear resistance. This datasheet provides information on composition, hardness, and bend strength. It also includes information on high temperature performance. Filing Code: TS-779. Producer or source: Hitachi Metals America Ltd.
Journal Articles
BÖHLER S700: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (10): TS-778.
Published: 01 October 2019
Abstract
View articletitled, BÖHLER S700: High-Speed Steel
View
PDF
for article titled, BÖHLER S700: High-Speed Steel
Böhler (or Boehler) S700 tungsten-molybdenum high-speed tool steel has good wear resistance and red hardness. This datasheet provides information on composition and physical properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-778. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.
Journal Articles
YSS HAP40: P/M High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (9): TS-775.
Published: 01 September 2019
Abstract
View articletitled, YSS HAP40: P/M High-Speed Steel
View
PDF
for article titled, YSS HAP40: P/M High-Speed Steel
YSS HAP40 is a powder metallurgy high-speed tool steel with very high hardness and toughness. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-775. Producer or source: Hitachi Metals America Ltd.
Journal Articles
BÖHLER S705: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (9): TS-776.
Published: 01 September 2019
Abstract
View articletitled, BÖHLER S705: High-Speed Steel
View
PDF
for article titled, BÖHLER S705: High-Speed Steel
Böhler (or Boehler) S705 is a cobalt alloyed, tungsten-molybdenum high-speed steel. Applications include turning and planing tools of all types, milling cutters,taps, twist drills, woodworking tools, and cold work tools. See also Alloy Digest TS-761, April 2019. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-776. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.
Journal Articles
BÖHLER S500: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (8): TS-772.
Published: 01 August 2019
Abstract
View articletitled, BÖHLER S500: High-Speed Steel
View
PDF
for article titled, BÖHLER S500: High-Speed Steel
Böhler (or Boehler) S500 is a conventional cobalt-molybdenum high-speed steel for applications in machining. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on forming. Filing Code: TS-772. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.
Journal Articles
YSS HAP10: Cold-Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (8): TS-773.
Published: 01 August 2019
Abstract
View articletitled, YSS HAP10: Cold-Work Tool Steel
View
PDF
for article titled, YSS HAP10: Cold-Work Tool Steel
YSS HAP10 is a powder metallurgy high-speed tool steel with very high toughness for cold forging dies and fine blanking dies. This datasheet provides information on composition, physical properties, and hardness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-773. Producer or source: Hitachi Metals America Ltd.
Journal Articles
BÖHLER S404: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (7): TS-769.
Published: 01 July 2019
Abstract
View articletitled, BÖHLER S404: High-Speed Steel
View
PDF
for article titled, BÖHLER S404: High-Speed Steel
Böhler (or Boehler) S404 is a conventional, economical, high-speed steel for applications in machining. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming. Filing Code: TS-769. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.
Journal Articles
YSS HAP5R: Cold Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (7): TS-770.
Published: 01 July 2019
Abstract
View articletitled, YSS HAP5R: Cold Work Tool Steel
View
PDF
for article titled, YSS HAP5R: Cold Work Tool Steel
YSS HAP5R is a powder metallurgy high-speed tool steel with very high toughness. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing Code: TS-770. Producer or source: Hitachi Metals America Ltd.
Journal Articles
YSS YXR3: Cold-work tool steel
Available to Purchase
Alloy Digest (2019) 68 (6): TS-768.
Published: 01 June 2019
Abstract
View articletitled, YSS YXR3: Cold-work tool steel
View
PDF
for article titled, YSS YXR3: Cold-work tool steel
YSS YXR3 is a matrix high-speed tool steel for general use. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-768. Producer or source: Hitachi Metals Ltd, Hitachi Metals America Ltd.
Journal Articles
BÖHLER S401: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (6): TS-766.
Published: 01 June 2019
Abstract
View articletitled, BÖHLER S401: High-Speed Steel
View
PDF
for article titled, BÖHLER S401: High-Speed Steel
Böhler (or Boehler) S401 tungsten-molybdenum HSS material has high toughness and cutting properties. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-766. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.
Journal Articles
BÖHLER S400: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (5): TS-765.
Published: 01 May 2019
Abstract
View articletitled, BÖHLER S400: High-Speed Steel
View
PDF
for article titled, BÖHLER S400: High-Speed Steel
Böhler (or Boehler) S400 is a conventional high-speed steel for applications in machining. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming. Filing Code: TS-765. Producer or source: Voestalpine High Performance Metals Corporation.
Journal Articles
BÖHLER S705: High-Speed Steel
Available to Purchase
Alloy Digest (2019) 68 (4): TS-761.
Published: 01 April 2019
Abstract
View articletitled, BÖHLER S705: High-Speed Steel
View
PDF
for article titled, BÖHLER S705: High-Speed Steel
Böhler (or Boehler) S705 is cobalt alloyed, tungsten-molybdenum high-speed steel possessing high hardness, excellent cutting properties, high red hardness, and good toughness. See also Alloy Digest TS-776, September 2019. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-761. Producer or source: Voestalpine High Performance Metals Corporation.
Journal Articles
YSS YXM1: Cold Work Tool Steel
Available to Purchase
Alloy Digest (2019) 68 (4): TS-762.
Published: 01 April 2019
Abstract
View articletitled, YSS YXM1: Cold Work Tool Steel
View
PDF
for article titled, YSS YXM1: Cold Work Tool Steel
High-speed tool steel with high-abrasion resistance and toughness for extended life. This datasheet provides information on composition, physical properties, hardness, and bend strength. It also includes information on heat treating. Filing Code: TS-762. Producer or source: Hitachi Metals America Ltd.
1