Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 160
Martensitic stainless steel
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (2022) 71 (12): SS-1354.
Published: 01 December 2022
Abstract
View article
PDF
CarTech 410 is a martensitic stainless steel that is suitable for highly stressed parts where corrosion resistance, good strength, and ductility are needed. This alloy can be used up to 650 °C (1200 °F) where resistance to scaling and oxidation is required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1354. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
Abstract
View article
PDF
Zapp Ergste 1.4028YN is a medium-carbon, 13% Cr, martensitic stainless steel that is designed for medical applications requiring high strength and hardness along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1326. Producer or Source: Zapp AG.
Journal Articles
Alloy Digest (2020) 69 (7): SS-1323.
Published: 01 July 2020
Abstract
View article
PDF
Zapp Ergste 1.4035YU is a medium-carbon, 13% chromium, free-cutting martensitic stainless steel that is designed for applications requiring high strength and hardness, along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1323. Producer or source: Zapp AG.
Journal Articles
Alloy Digest (2020) 69 (7): SS-1321.
Published: 01 July 2020
Abstract
View article
PDF
CarTech 420 is a hardenable, 13% chromium, martensitic stainless steel with higher strength and hardness, and better wear resistance than Type 410 stainless steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1321. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2020) 69 (6): SS-1320.
Published: 01 June 2020
Abstract
View article
PDF
Zapp Ergste 1.4034YK is a medium-carbon, 13.5% Cr, martensitic stainless steel that is designed for applications requiring high strength and hardness, along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1320. Producer or source: Zapp AG.
Journal Articles
Alloy Digest (2020) 69 (3): SS-1316.
Published: 01 March 2020
Abstract
View article
PDF
Sandmeyer Alloy 410 (UNS S41000) is a general purpose 12% chromium martensitic stainless steel that can be heat treated to obtain a wide range of mechanical properties. This alloy possesses good corrosion resistance along with high strength and hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1316. Producer or source: Sandmeyer Steel Company.
Journal Articles
Alloy Digest (2020) 69 (2): SS-1315.
Published: 01 February 2020
Abstract
View article
PDF
CarTech 1.4418 Stainless is a low-carbon, chromium-nickel-molybdenum martensitic stainless steel that is specially designed for those applications requiring high mechanical properties combined with improved corrosion resistance relative to traditional martensitic steels. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1315. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (2019) 68 (2): SS-1303.
Published: 01 February 2019
Abstract
View article
PDF
Sandvik 13C26 Medical Strip is martensitic stainless strip steel that has very good wear resistance. One important use is surgical blades. This datasheet provides information on composition, physical properties, and hardness as well as fatigue. It also includes information on wear resistance as well as heat treating. Filing Code: SS-1303. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (2018) 67 (12): SS-1300.
Published: 01 December 2018
Abstract
View article
PDF
UGI 4542 AIR is a martensitic precipitation hardening stainless steel with strong corrosion resistance and high mechanical performance. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1300. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2018) 67 (11): SS-1298.
Published: 01 November 2018
Abstract
View article
PDF
Sandvik APM 9980 is a low-carbon martensitic stainless steel with high mechanical properties. APM 9980 is a martensitic stainless steel specially designed for those applications requiring high mechanical properties combined with improved corrosion resistance relative to traditional martensitic steels. Note: This material is made by hot isostatic pressing of components. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1298. Producer or source: Sandvik Materials Technology and Sandvik AB Sweden.
Journal Articles
Alloy Digest (2018) 67 (10): SS-1296.
Published: 01 October 2018
Abstract
View article
PDF
UGI 4418 AIR is a martensitic stainless steel with strong corrosion resistance and mechanical performance. It is used for parts requiring a combination of high strength and high toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: SS-1296. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2018) 67 (8): SS-1292.
Published: 01 August 2018
Abstract
View article
PDF
UGI 4418 is a martensitic stainless steel with excellent corrosion resistance in aggressive environments combined with good mechanical properties, including toughness. It exhibits excellent cryogenic properties. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance, corrosion and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1292. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2018) 67 (5): SS-1287.
Published: 01 May 2018
Abstract
View article
PDF
UGI 4313 (EN 10083-3 , No. 1.4313) is a martensitic stainless steel with low carbon for good impact strength and corrosion resistance. It has good mechanical properties and impact strength, and a corrosion resistance superior to that of conventional martensitic stainless steel grades with a high carbon content. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1287. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2018) 67 (2): SS-1280.
Published: 01 February 2018
Abstract
View article
PDF
UGI 4545 Air is a precipitation hardening martensitic stainless steel designed for aerospace applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1280. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2018) 67 (1): SS-1275.
Published: 01 January 2018
Abstract
View article
PDF
UGI 4116N is a martensitic stainless steel with high carbon and nitrogen for hardness and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1275. Producer or source: Schmolz + Bickenbach USA Inc..
Journal Articles
Alloy Digest (2017) 66 (4): SS-1261.
Published: 01 April 2017
Abstract
View article
PDF
Superplast is a plastic mold steel with a high chromium content for corrosion resistance and a high sulfur content for good machinability. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1261. Producer or source: International Mold Steel Inc..
Journal Articles
Alloy Digest (2016) 65 (11): SS-1254.
Published: 01 November 2016
Abstract
View article
PDF
Vallourec VM 125 13Cr SS is a 13Cr super martensitic steel for use in oil country tubular goods as a material suitable for sour service. The CY version offers corrosion and SCC resistance on a greater usage domain than API L80-13Cr in terms of temperature and chloride content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1254. Producer or source: Vallourec USA Corporation.
Journal Articles
Alloy Digest (2016) 65 (10): SS-1251.
Published: 01 October 2016
Abstract
View article
PDF
Vallourec VM 110 13Cr SSCY is a 13Cr super martensitic steel for use in oil country tubular goods as a material suitable for sour service. The CY version offers corrosion and SCC resistance on a greater usage domain than API L80-13Cr in terms of temperature, H2S, and chloride content. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1251. Producer or source: Vallourec USA Corporation.
Journal Articles
Alloy Digest (2016) 65 (2): SS-1238.
Published: 01 February 2016
Abstract
View article
PDF
Outokumpu Type 630 is a martensitic age hardenable alloy of composition 17Cr-4Ni. The alloy has high strength and corrosion resistance similar to that of Type 304 stainless steel. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1238. Producer or source: Outokumpu High Performance Stainless.
Journal Articles
Alloy Digest (2015) 64 (6): SS-1212.
Published: 01 June 2015
Abstract
View article
PDF
AK 420 martensitic stainless steel has good corrosion resistance with increased strength over other 400 martensitic stainless steels. The alloy is magnetic. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1212. Producer or source: AK Steel Corporation.