Skip Nav Destination
Close Modal
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Date
Availability
1-20 of 43
Cu (Copper)
Close
Tin bronze
Close
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
WIELAND B31: Cu-2Sn-0.1Fe-0.03P Alloy
Available to Purchase
Alloy Digest (2021) 70 (11): Cu-926.
Published: 01 November 2021
Abstract
View articletitled, WIELAND B31: Cu-2Sn-0.1Fe-0.03P Alloy
View
PDF
for article titled, WIELAND B31: Cu-2Sn-0.1Fe-0.03P Alloy
Wieland B31 (CuSn2Fe0.1P) is a copper-tin-iron-phosphorus alloy (tin bronze) with coherent precipitates. The lower tin content with small amounts of iron and phosphorus results in an electrical conductivity of at least 30% IACS. Precipitates of iron and phosphorus stabilize the structure, increase the strength, and improve the softening characteristics. Wieland B31 possesses the right combination of formability, conductivity, strength, and stress relaxation resistance to be used for automotive applications at relatively high ambient temperatures. In addition, its strength is similar to that of a 4% tin bronze. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Cu-926. Producer or source: Wieland-Werke AG.
Journal Articles
CONCAST C89325: Copper-Casting Alloy
Available to Purchase
Alloy Digest (2019) 68 (8): Cu-893.
Published: 01 August 2019
Abstract
View articletitled, CONCAST C89325: Copper-Casting Alloy
View
PDF
for article titled, CONCAST C89325: Copper-Casting Alloy
Concast C89325 is a lead-free casting alloy that can be interchangeable with C937 (Alloy Digest Cu-421, August 1981). C89325 is classified as a bismuth tin bronze. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as machining. Filing Code: Cu-893. Producer or source: Concast Metal Products Company.
Journal Articles
CONCAST C89833: Copper Casting Alloy
Available to Purchase
Alloy Digest (2019) 68 (7): Cu-891.
Published: 01 July 2019
Abstract
View articletitled, CONCAST C89833: Copper Casting Alloy
View
PDF
for article titled, CONCAST C89833: Copper Casting Alloy
Concast C89833 is a lead-free casting alloy that can be interchangeable with C836 (Alloy Digest Cu-317, August 1976). C89833 is classified as a bismuth tin bronze. See also Federalloy I-844, Alloy Digest Cu-611, March 1997. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: Cu-891. Producer or source: Concast Metal Products Company.
Journal Articles
CONCAST C89831: Copper Casting Alloy
Available to Purchase
Alloy Digest (2019) 68 (6): Cu-889.
Published: 01 June 2019
Abstract
View articletitled, CONCAST C89831: Copper Casting Alloy
View
PDF
for article titled, CONCAST C89831: Copper Casting Alloy
Concast C89831 is a lead-free casting alloy that can be interchangeable with C844 (Alloy Digest Cu-349, March 1978). C89831 is classified as a bismuth tin bronze. This datasheet provides information on composition, physical properties, and elasticity. Filing Code: Cu-889. Producer or source: Concast Metal Products Company.
Journal Articles
WIELAND-G07: Cast Leaded Tin Bronze
Available to Purchase
Alloy Digest (2018) 67 (3): Cu-869.
Published: 01 March 2018
Abstract
View articletitled, WIELAND-G07: Cast Leaded Tin Bronze
View
PDF
for article titled, WIELAND-G07: Cast Leaded Tin Bronze
Wieland-G07 is a cast high leaded tin bronze subject to medium stress in slide bearing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fatigue. It also includes information on low temperature performance as well as heat treating and joining. Filing Code: Cu-869. Producer or source: Wieland Metals Inc..
Journal Articles
LUVATA C50725: Tin-Bronze
Available to Purchase
Alloy Digest (2010) 59 (6): Cu-783.
Published: 01 June 2010
Abstract
View articletitled, LUVATA C50725: Tin-Bronze
View
PDF
for article titled, LUVATA C50725: Tin-Bronze
Luvata C50725, nominally CuSn2Zn 2.2 Fe 0.1P, is a common tin bronze with good stress relaxation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-783. Producer or source: Luvata Sales (USA) Inc.
Journal Articles
LUVATA C50715: Tin Bronze
Available to Purchase
Alloy Digest (2010) 59 (2): Cu-779.
Published: 01 February 2010
Abstract
View articletitled, LUVATA C50715: Tin Bronze
View
PDF
for article titled, LUVATA C50715: Tin Bronze
Luvata C50715 is a very common and frequently used alloy. The 2% Sn and coherent precipitates improve properties. It is often called CuSn2Fe0.1P. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. and bend strength. It also includes information on forming. Filing Code: CU-779. Producer or source: Luvata Sales (USA) Inc.
Journal Articles
FEDERALLOY III-937: Machinable Lead-Free Bronze Casting Alloy
Available to Purchase
Alloy Digest (1997) 46 (2): Cu-610.
Published: 01 February 1997
Abstract
View articletitled, FEDERALLOY III-937: Machinable Lead-Free Bronze Casting Alloy
View
PDF
for article titled, FEDERALLOY III-937: Machinable Lead-Free Bronze Casting Alloy
Federalloy III-937 (C89325) is a lead-free bronze casting alloy that is machinable by alloying additions of bismuth. The alloy is designed for replacement of UNS C93700. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, machining, and joining. Filing Code: CU-610. Producer or source: Federal Metal Company.
Journal Articles
MAGNOLIA B-1: Lead-Free Machinable Bronze Casting Alloy
Available to Purchase
Alloy Digest (1997) 46 (1): Cu-609.
Published: 01 January 1997
Abstract
View articletitled, MAGNOLIA B-1: Lead-Free Machinable Bronze Casting Alloy
View
PDF
for article titled, MAGNOLIA B-1: Lead-Free Machinable Bronze Casting Alloy
Magnolia B-1 is a lead-free copper alloy. It machines easier than the leaded SAE 660 alloy that it was designed to duplicate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, machining, and joining. Filing Code: CU-609. Producer or source: I. Schumann Company.
Journal Articles
COPPER ALLOY No. C91000: Cast Copper Tin Alloy
Available to Purchase
Alloy Digest (1987) 36 (12): Cu-531.
Published: 01 December 1987
Abstract
View articletitled, COPPER ALLOY No. C91000: Cast Copper Tin Alloy
View
PDF
for article titled, COPPER ALLOY No. C91000: Cast Copper Tin Alloy
Copper Alloy No. C91000 is a cast copper-tin alloy which also is known by names formerly used (but not recommended): 197, Tin Bronze and 85-14-0-1. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Its uses include piston rings and bearings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-531. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C94500: High Leaded Medium Bronze
Available to Purchase
Alloy Digest (1987) 36 (9): Cu-528.
Published: 01 September 1987
Abstract
View articletitled, COPPER ALLOY No. C94500: High Leaded Medium Bronze
View
PDF
for article titled, COPPER ALLOY No. C94500: High Leaded Medium Bronze
Copper Alloy No. C94500 is a cast bronze containing nominally 73% copper, 20% lead and 7% tin. It has excellent machinability, good casting characteristics, low strength and good resistance to corrosion. It is used for bearings, locomotive wearing parts and for corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-528. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C91700: Copper Tin Nickel Casting Alloy
Available to Purchase
Alloy Digest (1986) 35 (12): Cu-519.
Published: 01 December 1986
Abstract
View articletitled, COPPER ALLOY No. C91700: Copper Tin Nickel Casting Alloy
View
PDF
for article titled, COPPER ALLOY No. C91700: Copper Tin Nickel Casting Alloy
Copper Alloy No. C91700 is a medium strength casting alloy. Formerly it was known as Nickel Gear Bronze and 861/2-12- 0-0-11/2; these names are no longer recommended. It has a good combination of strength, ductility and resistance to corrosion and wear. Its typical tensile strength is 60,000 psi in the as-cast condition. Typical applications include gears and worm wheels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-519. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C90900: Cast Copper Tin Alloy
Available to Purchase
Alloy Digest (1985) 34 (3): Cu-494.
Published: 01 March 1985
Abstract
View articletitled, COPPER ALLOY No. C90900: Cast Copper Tin Alloy
View
PDF
for article titled, COPPER ALLOY No. C90900: Cast Copper Tin Alloy
Copper Alloy No. C90900 is a cast copper-tin alloy which also is known by names formerly used (but not recommended): Tin Bronze, 199 and 87-13-0-0. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Its uses include bearings, bushings, valves, nuts and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-494. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C92800: Leaded Tin Bronze
Available to Purchase
Alloy Digest (1985) 34 (1): Cu-490.
Published: 01 January 1985
Abstract
View articletitled, COPPER ALLOY No. C92800: Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C92800: Leaded Tin Bronze
Copper Alloy No. C92800 is a cast bronze containing nominally 16% tin and 5% lead. Former commercial names (not recommended) are (1) 295, (2) Leaded Tin Bronze, (3) Ring Metal and (4) 79-16-5-0. It has excellent machinability, moderate strength and good resistance to corrosion. A typical use is piston rings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-490. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C93900: High Leaded Tin Bronze
Available to Purchase
Alloy Digest (1984) 33 (11): Cu-487.
Published: 01 November 1984
Abstract
View articletitled, COPPER ALLOY No. C93900: High Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C93900: High Leaded Tin Bronze
Copper Alloy No. C93900 is a cast bronze of fairly low strength. It has good machinability and good resistance to corrosion. Its commercial names formerly used (not recommended) are: (1) High-Leaded Tin Bronze and (2) 79-6-15. Among its uses are bearings for general service and pump bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-487. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-475, April 1984.
Journal Articles
COPPER ALLOY No. C92700: Cast Leaded Tin Bronze
Available to Purchase
Alloy Digest (1984) 33 (5): Cu-477.
Published: 01 May 1984
Abstract
View articletitled, COPPER ALLOY No. C92700: Cast Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C92700: Cast Leaded Tin Bronze
Copper Alloy No. C92700 is a cast copper-base alloy; it formerly was known as 88-10-2-0 alloy. It is characterized by a good combination of machinability, strength and resistance to corrosion. Among its many uses are bearings, pump impellers, piston rings and valve parts that are subject to liquid and or gas pressure and, therefore, must be sound (free from defects). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-477. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C93900: High Leaded Tin Bronze
Available to Purchase
Alloy Digest (1984) 33 (4): Cu-475.
Published: 01 April 1984
Abstract
View articletitled, COPPER ALLOY No. C93900: High Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C93900: High Leaded Tin Bronze
Copper Alloy No. C93900 is a cast copper-tin-lead alloy (bronze). It has good machinability, low strength and good resistance to corrosion. This alloy formerly was known by several commercial names (not recommended); they are: (1) High-Leaded Tin Bronze and (2) 79-6-15. It is produced only in the form of continuous castings and its uses include bearings, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-475. Producer or source: Copper alloy foundries. See also Alloy Digest Cu-487, November 1984.
Journal Articles
COPPER ALLOY No. C94300: High Leaded Tin Bronze
Available to Purchase
Alloy Digest (1984) 33 (1): Cu-470.
Published: 01 January 1984
Abstract
View articletitled, COPPER ALLOY No. C94300: High Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C94300: High Leaded Tin Bronze
Copper Alloy No. C94300 is a cast copper-tin-lead alloy (bronze). It is characterized by low hardness and strength, medium ductility, excellent machinability and good resistance to corrosion. Commercial names formerly used (but not recommended) are (1) Ingot No. 322, (2) Soft Bronze, (3) High-Leaded Tin Bronze and (4) 70-5-25. This alloy is recommended highly for high-speed bearings at light loads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-470. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C93800: High Leaded Tin Bronze
Available to Purchase
Alloy Digest (1983) 32 (10): Cu-464.
Published: 01 October 1983
Abstract
View articletitled, COPPER ALLOY No. C93800: High Leaded Tin Bronze
View
PDF
for article titled, COPPER ALLOY No. C93800: High Leaded Tin Bronze
Copper Alloy No. C93800 is a cast copper-tin-lead alloy (bronze). It is characterized by low strength, good machinability and good resistance to corrosion. Commercial names formerly used (not recommended) are (1) Anti-Acid Metal, (2) Ingot No. 319, (3) High-Leaded Tin Bronze and (4) 78-7-15. Its many applications include bearings, bushings, pump impellers and corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-464. Producer or source: Copper alloy foundries.
Journal Articles
COPPER ALLOY No. C90700: Cast Copper Tin Alloy
Available to Purchase
Alloy Digest (1983) 32 (6): Cu-460.
Published: 01 June 1983
Abstract
View articletitled, COPPER ALLOY No. C90700: Cast Copper Tin Alloy
View
PDF
for article titled, COPPER ALLOY No. C90700: Cast Copper Tin Alloy
Copper Alloy No. C90700 is a cast copper-tin alloy known also by names formerly used (but not recommended): Tin Bronze, 205 and 89-11. It is a medium-strength alloy and has a good combination of strength, ductility and resistance to corrosion. Among its many uses are gears, bearings, bushings and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-460. Producer or source: Copper alloy foundries.