Deutsche Edelstahlwerke Cryodur 2510 is a high-carbon, manganese-chromium-tungsten-vanadium alloy cold-work tool steel. This oil hardening type cold work tool steel offers a combination of high hardness, good wear resistance, and good cutting edge retention. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on heat treating. Filing Code: TS-838. Producer or source: Deutsche Edelstahlwerke Specialty Steel.