Alcoa Alclad 2029 sheet/plate is a high strength, high toughness, corrosion resistant alloy. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Al-453. Producer or source: Alcoa Aerospace and Automotive Products.