Abstract

Alloy KHP 7025 (UNS C70250) is a high-performance copper alloy with very high conductivity. Uses include connector springs, tabs, contact springs, switches, relays, and leadframes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-865. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.