Abstract

JFE880NH is a 900 MPa (131 ksi) microalloyed steel used as an alternative material, for a variety of uses, to 900 MPa grade quenched and tempered steels. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on forming. Filing Code: SA-633. Producer or source: JFE Steel America Inc..