Abstract

Diros 500 is a fine-grained pressure vessel steel delivered in two grades: one as high strength, the other for sour service. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-630. Producer or source: Dillinger Hütte GTS.