Abstract

Ansonia alloy C50700 is a low-tin phosphor bronze alloy with corrosion resistance combined with other properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-799. Producer or source: Ansonia Copper & Brass Inc..