NAS 600 is a nickel alloy with 14-17 chromium and has excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-688. Producer or source: Nippon Yakin Kogyo Company Ltd.