Kanthal 155 is a thermostatic bimetal and is recommended for use in the temperature range −20 to 350 deg C, −4 to 660 deg F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: FE-147. Producer or source: Kanthal AB.