Abstract

K MONEL is a corrosion-resistant wrought alloy of nickel, copper and aluminum. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-17. Producer or source: The International Nickel Company Inc..