Abstract

VAIRLOY is a manganese-chromium-molybdenum tool and die steel capable of being air-hardened at low temperatures with minimum distortion and deformation. It is strong, tough and wear resistant. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and machining. Filing Code: TS-6. Producer or source: Vulcan Crucible Steel Company.