HY-TEN-SL No. 1 is a close-grained, tough, homogeneous metal, having the non-corrosive properties of bronze and the strength of alloy steel. It has good wear resisting qualities under heavy or shock loads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-7. Producer or source: American Manganese Bronze Company.