Abstract

CRUCIBLE BETA III is a heat-treatable beta titanium alloy offering outstanding cold formability and simple heat treatment to high strengths. It is recommended for aircraft parts and fasteners. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, joining, and surface treatment. Filing Code: Ti-59. Producer or source: Crucible Steel Company of America, Titanium Division.