Abstract

CML-605 is a cobalt-base alloy having high strength, heat and oxidation resistance at elevated temperatures above 1600 F. It is recommended for gas turbine and jet engine components operating in the 1600 to 2000 F temperature range. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Co-60. Producer or source: Cannon-Muskegon Corporation.