CMN-155 is an austenitic iron-base alloy having high oxidation and heat resistance combined with good high temperature properties. It is recommended for jet engine and gas turbine components, high temperature fasteners, and rocket chambers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SS-212. Producer or source: Cannon-Muskegon Corporation.