Abstract

Titanium IA1-8V-5Fe is an all beta type titanium alloy recommended for high temperature fasteners. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-55. Producer or source: Reactive Metals Corporation.