Abstract

ELEKTRON Magnesium-ZTY is a wrought magnesium alloy that retains almost constant 0.1% yield strength of 22000 psi up to 190 C. It is hot formable, easily machined and fully weldable. It was developed for use at temperatures up to about 250 C (480 F). This datasheet provides information on composition, physical properties, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Mg-66. Producer or source: Magnesium Elektron Ltd.