Abstract

Hylite 60 is an alpha plus beta alloy having high tensile strength and good creep properties. It is suitable for compressor discs and blades and other highly stressed components up to 500 C. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-54. Producer or source: Jessop-Saville Ltd, Brightside Works.