Abstract

UNITEMP-1430MV is a martensitic high-chromium, molybdenum heat and corrosion resisting steel used for highly stressed parts involving service temperatures up to 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-199. Producer or source: Cyclops Corporation.