Abstract

EVERDUR-651 is a high-strength, corrosion-resistant copper-silicon alloy having good fabricating properties. It is non-magnetic and fatigue resistant. It is used for cold-headed bolts, hardware, marine fittings, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-179. Producer or source: Anaconda American Brass Company.