Abstract

DARWINS 18/8 W.P.D. is a titanium stabilized 18/8 type stainless steel being free of weld decay. It is recommended for welded equipment and structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-195. Producer or source: Darwin's Ltd.