Abstract

Republic RS-110C is a moderate strength highly weldable titanium alloy recommended for jet engine welded rings, aircraft skins, and structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-42. Producer or source: Republic Steel Corporation, Titanium Division.