Algo-Loy 1317 is a high-strength low-alloy structural steel for bolted and riveted construction. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-159. Producer or source: Algoma Steel Corporation Ltd.