Abstract

JESSOP-SAVILLE ZIRCONIUM Alloy has a high melting point and possesses excellent corrosion resistance coupled with low neutron absorption properties. It is equivalent to ZIRCALOY 2. It is recommended for pressurized water reactors. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zr-2. Producer or source: Jessop-Saville Ltd, Brightside Works.