Abstract

The SD group is part of the Densalloy family of materials, which are high-density alloys used for a variety of applications, from counterbalance weights to radiation shielding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: W-28. Producer or source: Tungsten Products, An Allegheny Technologies Company.