Abstract

Uddeholm Vanadis 8 SuperClean is a high-carbon, Cr-Mo-V, alloy cold work tool steel that is produced by the powder metallurgy process. It is suitable for very long run tooling where a combination of very high wear resistance and good chipping resistance is required. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-804. Producer or source: Uddeholms AB (a voestalpine company).