Abstract

Industeel D2 is an air-hardening, high-carbon (1.5%), high-chromium (12%), alloy cold-work tool steel that also contains molybdenum and vanadium. It is specifically designed to provide high abrasive wear resistance and high hardenability. This grade can be used for cutting and deformation tools submitted to high abrasive wear. It can be used when Type D3 tool steel shows an excessive sensitivity to cracking or chipping. This datasheet provides information on composition, physical properties, hardness, and elasticity. Filing Code: TS-791. Producer or source: Industeel France (a subsidiary of ArcelorMittal.