Abstract

Böhler K100 is a high-carbon, high-chromium (12%), alloy cold-work tool steel that is suitable for medium run tooling in applications where a very good abrasive wear resistance is needed but where demands on chipping resistance are small. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming and machining. Filing Code: TS-788. Producer or source: voestalpine Böhler Edelstahl GmbH & Co.