Abstract

Böhler (or Boehler) S705 is a cobalt alloyed, tungsten-molybdenum high-speed steel. Applications include turning and planing tools of all types, milling cutters,taps, twist drills, woodworking tools, and cold work tools. See also Alloy Digest TS-761, April 2019. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating and machining. Filing Code: TS-776. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.