YSS YXR3 is a matrix high-speed tool steel for general use. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: TS-768. Producer or source: Hitachi Metals Ltd, Hitachi Metals America Ltd.